Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer A. Schulman, Inc.
Trade Name POLYTROPE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for molding large automotive parts, such as fascias and air dams. TPP 510 is UV stable, paintable and pigmentable.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Linear Mold Shrinkage 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
Melt Index of Compound 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength at Break 20.7 MPa
3000 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Modulus 0.689 GPa
100 ksi
ASTM D790
Gardner Impact 36.0 J

@Temperature -30.0 °C
26.6 ft-lb

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Brittleness Temperature -45.0 °C
-49.0 °F
Users viewing this material also viewed the following: