Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loxim 830 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Talc Filler , Polypropylene, Flame Retardant
Manufacturer Loxim Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loxim 830 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.05 - 1.15 g/cc
1.05 - 1.15 g/cc
ASTM D792
Filler Content 30 %
30 %
Linear Mold Shrinkage 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 - 30.0 MPa
4060 - 4350 psi
ASTM D683
Flexural Modulus 2.40 - 2.60 GPa
348 - 377 ksi
ASTM D790
Izod Impact, Notched 0.300 - 0.400 J/cm
0.562 - 0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 - 125 °C
239 - 257 °F
ASTM D1525, HDT Method B
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Copyright © lookpolymers.com All Rights Reserved