Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Nilit (formerly Frisetta Polymer)
Trade Name FRIANYL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit FRIANYL B63 W-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Water Absorption 1.3 - 2.3 %
1.3 - 2.3 %
ISO 62
Water Absorption at Saturation 5.5 - 7.5 %
5.5 - 7.5 %
ISO 62
Viscosity Measurement 145
145
Viscosity index; ISO 307
Linear Mold Shrinkage 0.0060 - 0.013 cm/cm
0.0060 - 0.013 in/in
FRISETTA Test Method
Mechanical Properties Metric English Comments
Ball Indentation Hardness 175 MPa
25400 psi
ISO 2039-1
Tensile Strength at Break 170 MPa
24700 psi
ISO 527
Elongation at Break 4.0 %
4.0 %
ISO 527
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527
Flexural Strength 220 MPa
31900 psi
ISO 178
Flexural Modulus 7.20 GPa
1040 ksi
ISO 178
Charpy Impact Unnotched 5.50 J/cm²
26.2 ft-lb/in²
DIN 53453
NB
NB
ISO 179/1eU
5.00 J/cm²

@Temperature -40.0 °C
23.8 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1eA
1.50 J/cm²
7.14 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ISO 3146 DSC
Maximum Service Temperature, Air 115 °C
239 °F
Continuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 93
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 575 V
575 V
CTI 100; IEC 112