Material Notes:
Description: SEQUEL® 1485 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, improved scratch and mar resistance, and excellent paintability and processability. Applications: Bumper fascias Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
ISO 1183
Linear Mold Shrinkage 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
as molded; ISO 294
0.010 - 0.013 cm/cm
0.010 - 0.013 in/in
after bake; ISO 294
Melt Flow 20 g/10 min
20 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 1.08 GPa
157 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Thermal Properties Metric English Comments
CTE, linear 65.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
36.1 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228
Users viewing this material also viewed the following: