Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00150 - 0.0100 cm/cm
0.00150 - 0.0100 in/in
Average value: 0.00450 cm/cm Grade Count:7
Overview of materials for Polycarbonate/Polysulfone Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o..
Linear Mold Shrinkage 0.00150 - 0.00300 cm/cm
0.00150 - 0.00300 in/in
Average value: 0.00213 cm/cm Grade Count:6
Overview of materials for Phenolic, Resole, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Linear Mold Shrinkage 0.00150 - 0.0190 cm/cm
0.00150 - 0.0190 in/in
Average value: 0.00822 cm/cm Grade Count:64
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
Linear Mold Shrinkage 0.00150 - 0.0350 cm/cm
0.00150 - 0.0350 in/in
Average value: 0.0158 cm/cm Grade Count:263
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Linear Mold Shrinkage 0.00150 - 0.0280 cm/cm
0.00150 - 0.0280 in/in
Average value: 0.0124 cm/cm Grade Count:100
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Linear Mold Shrinkage 0.00150 - 0.0500 cm/cm
0.00150 - 0.0500 in/in
Average value: 0.00641 cm/cm Grade Count:111
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage 0.00150 - 0.0240 cm/cm
0.00150 - 0.0240 in/in
Average value: 0.0101 cm/cm Grade Count:23
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
Linear Mold Shrinkage 0.00150 - 0.00700 cm/cm
0.00150 - 0.00700 in/in
Average value: 0.00401 cm/cm Grade Count:86
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..
Linear Mold Shrinkage 0.00150 - 0.00800 cm/cm
0.00150 - 0.00800 in/in
Average value: 0.00526 cm/cm Grade Count:248
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Linear Mold Shrinkage 0.00150 - 0.0120 cm/cm
0.00150 - 0.0120 in/in
Average value: 0.00433 cm/cm Grade Count:33
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..
Linear Mold Shrinkage 0.00150 - 0.00800 cm/cm
0.00150 - 0.00800 in/in
Average value: 0.00356 cm/cm Grade Count:13
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..
Linear Mold Shrinkage 0.00150 - 0.0200 cm/cm
0.00150 - 0.0200 in/in
Average value: 0.0119 cm/cm Grade Count:53
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..