Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Statiblend® PP CO 99074

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Techmer ES
Trade Name Statiblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Statiblend® PP CO 99074.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFeature: Copolymer and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792
Melt Flow 7.0 g/10 min

@Load 10.0 kg,
Temperature 230 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Yield 100 %
100 %
ASTM D638
Flexural Yield Strength 35.2 MPa
5100 psi
ASTM D790
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm
16.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 166 °C
330 °F
Deflection Temperature at 0.46 MPa (66 psi) 91.7 °C
197 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.7 °C
125 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 50 ohm-cm
50 ohm-cm
ASTM D257
Surface Resistance 200 ohm
200 ohm
ASTM D257
Copyright © lookpolymers.com All Rights Reserved