CENTROPLAST CENTROMID 12 LE soft Polyamide 12 LE soft

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, Extrusion/Tubing Grade
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTROMID
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTROMID 12 LE soft Polyamide 12 LE soft.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.60 %
0.60 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 1.1 %
1.1 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
v = 5 mm/min; ISO 527-2
Tensile Strength, Yield 20.0 MPa
2900 psi
v = 50 mm/min; ISO 527-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-2
Tensile Modulus 0.350 GPa
50.8 ksi
ISO 527-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched NB
NB
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C

@Temperature 20.0 °C
55.6 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Melting Point 178 °C
352 °F
10K/min; ISO 3146
Maximum Service Temperature, Air 80.0 - 100 °C
176 - 212 °F
Long Term
130 °C
266 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
104 °F
ISO 75-2
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
HB

@Thickness 6.00 mm
HB

@Thickness 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 43.0 kV/mm
1090 kV/in
in transformer oil; IEC 60243-1
Comparative Tracking Index 575 V
575 V
IEC 60112
Descriptive Properties Value Comments
Food Compliance yes
BGVV
yes
FD A