Material Notes:
DuPont™ Appeel 20D855 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature range to a number of container materials including PET, PVC, PS and PP. Appeel 20D855 is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene resins. Appeel® 20D855 resin complies with Food and Drug Administration Regulation 21 FDA Status Information CFR 177.1340 - - Ethylene-methyl acrylate copolymer resins, subject to the limitations and requirements therein. This Regulation describes polymers that may be used in contact with food, subject to the finished food-contact article meeting the extractive limitations under the intended conditions of use, as shown in paragraph (b) of the Regulation.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792, ISO 1183
Melt Flow 7.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 92.0 °C
198 °F
ASTM D3418, ISO 3146
Vicat Softening Point 54.0 °C
129 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 300 °C
<= 572 °F
Feed Temperature 140 °C
284 °F
Blown Film Coextrusion
160 °C
320 °F
Extrusion Coating
Zone 2 150 °C
302 °F
Blown Film Coextrusion
210 °C
410 °F
Extrusion Coating
Zone 3 160 °C
320 °F
Blown Film Coextrusion
260 °C
500 °F
Extrusion Coating
Zone 4 180 °C
356 °F
Blown Film Coextrusion
285 °C
545 °F
Extrusion Coating
Zone 5 180 °C
356 °F
Blown Film Coextrusion
285 °C
545 °F
Extrusion Coating
Adapter Temperature 180 °C
356 °F
Blown Film Coextrusion
285 °C
545 °F
Extrusion Coating
Die Temperature 170 °C
338 °F
Blown Film Coextrusion
285 °C
545 °F
Extrusion Coating
Melt Temperature 160 - 185 °C
320 - 365 °F
Blown Film Coextrusion
235 - 285 °C
455 - 545 °F
Extrusion Coating