Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.00 - 1.04 g/cc | 0.0361 - 0.0376 lb/in³ | Average value: 1.02 g/cc Grade Count:26 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0377 lb/in³ | |
Lord Adhesives 204 Semi-Flexible, Medium Cure, High Viscosity Acrylic Adhesive Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f.. |
|||
Density | 0.989 - 1.04 g/cc | 0.0357 - 0.0376 lb/in³ | 309-2D Hardener |
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh.. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0377 lb/in³ | Curative 44 |
Lord Adhesives Chemlok® 485/Curative 44 Adhesive LORD Chemlok® 485/Curative 44 adhesive is a two component adhesive system used for insert mold bonding of PVC and Alcryn® to substrates such as metal, rubber and other thermoplastic elastomers.. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0376 lb/in³ | |
Silikony Polskie Silpasta A Silicone Paste Vaseline consistency, slightly thixotropicAntiadhesive agent used in thermoplastic and thermosetting processing to paste ground joints, rubber gaskets, etc. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0376 lb/in³ | |
Silikony Polskie Silpasta E Silicone Paste Vaseline consistency, thixotropicElectric insulation to paste insulators, conductor connection, cable boxes in environment of high humidity or dustiness. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0376 lb/in³ | |
Silikony Polskie Silpasta EM Silicone Paste Vaseline consistency, thixotropicElectric insulation for mechanical application of protective layers on electric devices and connections. |
|||
Density | 1.00 - 1.04 g/cc | 0.0361 - 0.0376 lb/in³ | RP-0549 |
Solvay AG-RHOâ„¢ FM 3896 Surfactant Description: Agricultural Foam Marker Concentrate. Very low alcohol content. Performs well in hard water up to 1000 ppmChemical Name: FOAM MARKER CONCENTRATE CAS: 111-76-2, 64-17-5 Solubility in Wat.. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0376 lb/in³ | approximation |
Struktol STRUKSILON 8101 Silicone Stabilizer for PU-Rigid Foam STRUKSILON 8101 is used as a silicone stabilizer for production of polyurethane rigid foam. It is especially recommended for the use in PU-1- or PU-2-component spray foam applications.Applications: .. |
|||
Density | 0.960 - 1.04 g/cc | 0.0347 - 0.0376 lb/in³ | RP-0549 |
Solvay RHODATERGE® MULTIGREEN II Surfactant Description: Rhodaterge® Rhodaterge® Multigreen II is a general purpose Green Concentrate. It provides excellent oily soil removal for household, industrial and institutional products. It sis .. |
|||
Density | 0.900 - 1.04 g/cc | 0.0325 - 0.0376 lb/in³ | Average value: 0.920 g/cc Grade Count:278 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |
|||
Density | 0.930 - 1.04 g/cc | 0.0336 - 0.0376 lb/in³ | Average value: 0.957 g/cc Grade Count:16 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimu.. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0376 lb/in³ | |
Silikony Polskie Silpasta Z Silicone Paste A consistency of hard VaselineLubricating agent to dampen vibrations in transmission gears and other mobile element made of plastic. |
|||
Density | 1.01 - 1.04 g/cc | 0.0365 - 0.0376 lb/in³ | |
Solvay RHODASURF® BC-840 Surfactant Chemical Name: TRIDECYL ALCOHOL ETHOXYLATEDCAS: 78330-21-9Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODASURF BC-840 is used for the following applications: f.. |
|||
Density | 1.03 - 1.04 g/cc | 0.0372 - 0.0376 lb/in³ | |
Solvay RHODASURF® ON-870 Surfactant Description: Rhodasurf® ON 870 is Ethoxylated Oleyl Alcohol. It is low foaming emulsifier. It is good wetting agent, dispersant, and detergent.Chemical Name: ETHOXYLATED OLEYL ALCOHOLCAS: 9004-98-2.. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0377 lb/in³ | |
Lord Adhesives 201 Semi-Flexible, Medium Cure, Medium Viscosity Acrylic Adhesive Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f.. |
|||
Density | 0.886 - 1.04 g/cc | 0.0320 - 0.0376 lb/in³ | Average value: 0.905 g/cc Grade Count:61 |
Overview of materials for Polypropylene, Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values.. |