Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay ALKAMULS® OL 40 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ALKAMULS®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ALKAMULS® OL 40 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: POLYOXYETHYLENE SORBITOL HEXAOLEATECAS: 057171 – 56 – 9Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Emulsifier for paraffinic, naphtenic, vegetable and ester oils in water. Highly branched structure with a HLB of 10.2. Used in metal working fluids and water treatment applications.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
Iodine Absorption Number 88 - 100
88 - 100
[g l<sub>2</sub>/100 g]; RPG13
Thermal Properties Metric English Comments
Pour Point <= 0.000 °C
<= 32.0 °F
Flash Point >= 100 °C
>= 212 °F
Chemical Properties Metric English Comments
Total Acid Number 7.0 - 12
7.0 - 12
[mg KOH/g]; RPG03
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Yellow oily liquid
Composition Active content
1
Ionic Charge Nonionic
Saponification number 90-105 mg KOH/g
RPG05