| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Noryl EN110 PPE+HIPS (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
| Moisture Absorption at Equilibrium | 0.060 % | 0.060 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.15 % <br>@Temperature 23.0 °C |
0.15 % <br>@Temperature 73.4 °F |
ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | on tensile bar; SABIC Method |
| Melt Flow | 15 g/10 min <br>@Load 3.80 kg,<br> Temperature 280 °C |
15 g/10 min <br>@Load 8.38 lb,<br> Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, H358/30 | 87.0 MPa | 12600 psi | ISO 2039-1 |
| Tensile Strength at Break | 40.0 MPa | 5800 psi | 50 mm/min; ISO 527 |
| Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50 mm/min; ISO 527 |
| Elongation at Break | 30 % | 30 % | 50 mm/min; ISO 527 |
| Elongation at Yield | 3.0 % | 3.0 % | 50 mm/min; ISO 527 |
| Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
| Flexural Yield Strength | 60.0 MPa | 8700 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 2.00 GPa | 290 ksi | 2 mm/min; ISO 178 |
| Izod Impact, Notched (ISO) | 5.00 kJ/m² <br>@Temperature -30.0 °C |
2.38 ft-lb/in² <br>@Temperature -22.0 °F |
80*10*4; ISO 180/1A |
| 11.0 kJ/m² <br>@Temperature 23.0 °C |
5.23 ft-lb/in² <br>@Temperature 73.4 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 0.500 J/cm² <br>@Temperature -30.0 °C |
2.38 ft-lb/in² <br>@Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| 1.10 J/cm² <br>@Temperature 23.0 °C |
5.23 ft-lb/in² <br>@Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
| Deflection Temperature at 0.46 MPa (66 psi) | 100 °C | 212 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
| Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ISO 306 |
| 115 °C | 239 °F | Rate B/120; ISO 306 | |
| 120 °C | 248 °F | Rate A/50; ISO 306 | |
| Flammability, UL94 | HB <br>@Thickness 1.65 mm |
HB <br>@Thickness 0.0650 in |
UL 94 by SABIC-IP |
| Oxygen Index | 22 % | 22 % | LOI; ISO 4589 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ROA; IEC 60093 |
| Dielectric Constant | 2.6 <br>@Frequency 1.00e+6 Hz |
2.6 <br>@Frequency 1.00e+6 Hz |
IEC 60250 |
| 2.6 <br>@Frequency 50.0 - 60.0 Hz |
2.6 <br>@Frequency 50.0 - 60.0 Hz |
IEC 60250 | |
| Dielectric Strength | 19.0 kV/mm <br>@Thickness 3.20 mm |
483 kV/in <br>@Thickness 0.126 in |
in oil; IEC 60243-1 |
| Dissipation Factor | 0.0010 <br>@Frequency 1.00e+6 Hz |
0.0010 <br>@Frequency 1.00e+6 Hz |
IEC 60250 |
| 0.0040 <br>@Frequency 50.0 - 60.0 Hz |
0.0040 <br>@Frequency 50.0 - 60.0 Hz |
IEC 60250 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 75°C +/- 2°C | PASSES | IEC 60695-10-2 |