| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Lexan® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Lexan® LUX9616G PC (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
| Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.150 % | 0.150 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.35 % | 0.35 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm <br>@Thickness 3.20 mm |
0.0060 - 0.0080 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Melt Flow | 7.0 g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C |
7.0 g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F |
ASTM D1238 |
| Melt Index of Compound | 7.0 g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C |
7.0 g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 58.0 MPa | 8410 psi | 50 mm/min; ISO 527 |
| 65.0 MPa | 9430 psi | Type I, 50 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D638 |
| 62.0 MPa | 8990 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | 75 % | 75 % | 50 mm/min; ISO 527 |
| 80 % | 80 % | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Yield | 6.0 % | 6.0 % | Type I, 50 mm/min; ASTM D638 |
| 6.0 % | 6.0 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.23 GPa | 323 ksi | 1 mm/min; ISO 527 |
| 2.30 GPa | 334 ksi | 5 mm/min; ASTM D638 | |
| Flexural Strength | 95.0 MPa | 13800 psi | 12.5 mm/min; ISO 178 |
| Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 2.16 GPa | 313 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
| Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*3; ISO 180/1A |
| Dart Drop, Total Energy | 70.0 J <br>@Temperature 23.0 °C |
51.6 ft-lb <br>@Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 68.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| CTE, linear, Transverse to Flow | 67.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| Deflection Temperature at 1.8 MPa (264 psi) | 123 °C | 253 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 125 °C <br>@Thickness 3.20 mm |
257 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ASTM D1525 |
| UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | UL 746B |
| UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
| Flammability, UL94 | V-0 <br>@Thickness 1.50 mm |
V-0 <br>@Thickness 0.0591 in |
UL 94 |
| Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
| 850 °C | 1560 °F | IEC 60695-2-13 | |
| 960 °C <br>@Thickness 1.00 mm |
1760 °F <br>@Thickness 0.0394 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
| High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 125°C +/- 2°C | PASSES | IEC 60695-10-2 |