| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 2.16 GPa | 313 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| SABIC Innovative Plastics Cycolac® GX3800F ABS High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
| Flexural Modulus | 2.16 - 3.14 GPa | 313 - 455 ksi | Average value: 2.63 GPa Grade Count:6 |
| Overview of materials for PEN-PET This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent.. |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| SABIC Innovative Plastics Cycolac® EX58F ABS (Asia Pacific) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| SABIC Innovative Plastics Lexan® EXRL2032 PC (Asia Pacific) Lexan EXRL2032 is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS requir.. |
|||
| Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
50mm/min; ASTM D790 |
| LG Chemical Lupox® TE5000H PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
| Kotec Carbotex K-20UV30 Polycarbonate, General Purpose, UV Stability Grade UV stability, Ultra Low viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting covers, Safety products, E & E parts, Household applications, Leisure.. |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
| Kotec Carbotex K-20UVR Polycarbonate, General Purpose, UV Stability + Mold Release Grade Features: UV stability, Mold release, Low viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting Covers, Safety products, E & E parts, Household app.. |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
| Kotec Carbotex K-30 Polycarbonate, General Purpose Features: Standard, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household applications, Le.. |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
| Kotec Carbotex K-30UVR Polycarbonate, General Purpose, UV Stability + Mold Release Grade Features: UV stability, Mold release, Medium viscosityApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures/covers, Safety products, E & E parts, Household appl.. |
|||
| Flexural Modulus | 2.16 GPa @Thickness 3.20 mm |
313 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
| LG Chemical LUPOY GN1002FC PC, Halogen Free, Flame Retardant, High Impact Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 25232-40-0 and 139189-30-3Information .. |
|||
| Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
| LG Chemical TR300 MABS, Flame Retardant, Transparency Feature: Injection Molding, Flame Retardant, TransparencyApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9010-94-0 and 25713-60-4Information provided by LG Ch.. |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
| SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Asia Pacific) LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | 15 mm/min. ASTM D790 |
| Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Starex® PT-0180 ABS, Unreinforced Painting Grade Information provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D638 |
| Samsung Cheil Industries Starex® VH-0819 ABS, Unreinforced FR Flame-retardant high flow ABS that can be used for the exterior of large TV and OA devicesInformation provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® HI-1001BG PC/ABS, Metal Plating Grade PC/ABS material that can be used in automobile wheel cap and air-conditioner panelInformation provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® SC-1100R PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Starex® AS-0151BS ABS, Unreinforced Anti-static material that can be used in the housing of OA devices, IC, LSI carrier etc.Information provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Starex® TH-1100 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
| PlastxWorld CEVIAN® S1500 High Heat PC/ABS alloy These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
| Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
ASTM D-790 |
| Bhansali Engineering Abstron HR-59(M) ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
| Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
| Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
| Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
| Bhansali Engineering Abstron IM21G ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
| PlastxWorld CEVIAN® A1700 PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.Information provided by PlastxWorld Inc. |
|||
| Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
| Bhansali Engineering Abstron HI40I ABS Injection Molding Grade Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali |
|||
| Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
| Samyang Trirex® 3020R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020R is a high flow grade with added heat stabilizers and separating materials.Informa.. |
|||
| Flexural Modulus | 2.16 GPa @Thickness 3.20 mm |
313 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
| LG Chemical LUPOY NS5000C PC/ABS, High Impact Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
| Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
| Bhansali Engineering Abstron IM17V ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |
|||
| Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
| Bhansali Engineering Abstron IM17A TT ABS Injection Molding Grade High Flow, Medium ImpactInformation provided by Bhansali |
|||
| Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
| Bhansali Engineering Abstron IM21G ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |
|||