Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 35.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® LUX2289 PC
Lexan* LUX2289 resin is an injection molding grade with high light reflectance
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® LUX2289 PC (Europe-Africa-Middle East)
Lexan* LUX2289 resin is an injection molding grade with high light reflectance and UV stabilized
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature 20.0 °C
35.0 µin/in-°F
<br>@Temperature 68.0 °F
Covestro Makroblend® UT-408 Polycarbonate + Polyester Blend &nbsp;(discontinued **)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015,..
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
35.0 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP DFL34EH PC
LNP* LUBRICOMP* DFL34EH is a compound based on Polycarbonate containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Easy Molding, Healthcare, Wear Resistant.
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature 20.0 °C
35.0 µin/in-°F
<br>@Temperature 68.0 °F
Cookson Group Plaskon® AMC2 (132.203) Epoxy Molding Compound &nbsp;(discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound specifically formulated for packaging stress-sensitive devices in DIPs, SOICs, PLCCs and small QFPs. F..
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
35.0 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RFL449 PA 66
LNP* LUBRICOMP* RFL449 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Flame Retardant.
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
35.0 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA12
LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
35.0 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-kon DD0009XQ PC (Europe-Africa-Middle East)
LNP* Stat-Kon* DD0009XQ is a compound based on Polycarbonate containing Carbon Powder and Flame Retardant. Added features include Electrically Conductive, Flame Retardant and Easy Molding.This data..
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DD000CEX PC
LNP STAT-KON* DD000CEX is a compound based on Polycarbonate resin containing Carbon. Added features of this material include: Clean Compounding System. Easy Molding, Electrically Conductive.
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DD000CEX PC (Asia Pacific)
LNP* STAT-KON* DD000CEX is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System.
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature 25.6 - 93.3 °C
35.0 µin/in-°F
<br>@Temperature 78.0 - 200 °F
Diameter
Saint-Gobain Rulon® 957 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
35.0 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RC006XXH PA 66
LNP* THERMOCOMP* RC006XXH is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare.
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
35.0 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RX09411H PA 66
LNP* Thermocomp* RX09411H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare.
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
35.0 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP UX06003 PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UX06003 is a compound based on Polyphalamide resin containing Carbon Fiber. Added features include Electrically Conductive, Mold Release, Heat Stabilized.
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
35.0 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP VERTON MV00ES PP
LNP* VERTON* MV00ES is primarily a concentrate used for blending purposes. This is a 70% long glass fiber Polypropylene compound. Added features of this grade are: Heat Stabilized
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP
40% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited).
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Asia Pacific)
40% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited).
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
35.0 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP 9X02841 PBT+PC
LNP* Thermocmop* 9X02841 is a PBT/Polycarbonate blend containing proprietary fillers.
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
35.0 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP RC00A PA6.6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RC00A is a compound based on PA6.6 resin containing Carbon Fiber. Added features include: Electrically Conductive
CTE, linear, Transverse to Flow 63.0 - 65.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
35.0 - 36.1 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM E 831
SABIC Innovative Plastics LNP Verton RV008ESV PA 66
40% long glass fiber filled PA66 Verton Xtreme XCThis data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature 20.0 °C
35.0 µin/in-°F
<br>@Temperature 68.0 °F
Toyobo TS401 HS PPS, 40% Glass Fiber Reinforced
Key Feature: High toughness, high flow. Features high weld strength.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology d..
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature 20.0 °C
35.0 µin/in-°F
<br>@Temperature 68.0 °F
Toyobo TS401 PPS, 40% Glass Fiber Reinforced
Key Feature: General Purpose Grade - balanced characteristics suitable for a broad range of uses.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a spec..
CTE, linear, Transverse to Flow 63.0 µm/m-°C
35.0 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA) &nbsp;(Unverified Data**)
30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel..
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature 20.0 - 93.3 °C
35.0 µin/in-°F
<br>@Temperature 68.0 - 200 °F
Normal to Laminate
CIP Composites 200 Series Laminated Polymer Bearing Material
The 200 series consists of PTFE/polyester combination fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated ma..
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature 20.0 - 93.3 °C
35.0 µin/in-°F
<br>@Temperature 68.0 - 200 °F
Normal to Laminate
CIP Composites 100 Series Laminated Polymer Bearing Material
The 100 series consists of polyester fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated..
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
35.0 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM
Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva..
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
35.0 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RF007SXN PA 66
LNP* THERMOCOMP* RF007SXN is a Hydro-Stable, 35% Glass Fiber reinforced compound based on Nylon 66. Added features of this grade include: Heat Stabilized, NSF Listed.
CTE, linear, Transverse to Flow 63.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
35.0 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP VERTON RV00CEXS PA 66
LNP* VERTON* RV00CEXS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural.