| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 29.0 µm/m-°C | 16.1 µin/in-°F | ASTM D696 |
|
PolyOne Edgetek® PC-20GF/000 Polycarbonate (PC)
Information provided by PolyOne
|
|||
| CTE, linear, Parallel to Flow | 29.0 µm/m-°C | 16.1 µin/in-°F | ASTM D696 |
|
PolyOne Edgetek® PF-20GF/000 Polysulfone (PSU)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature 23.0 - 60.0 °C
|
16.1
µin/in-°F <br>@Temperature 73.4 - 140 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL146 PC (Europe-Africa-Middle East)
LNP* Lubricomp* DFL146 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Flame Retardant.
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature -30.0 - 30.0 °C
|
16.1
µin/in-°F <br>@Temperature -22.0 - 86.0 °F
|
ASTM D696 |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL38 PC
LNP* Lubricomp* DFL-4038 is a Polycarbonate containing 40% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated.
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature -30.0 - 30.0 °C
|
16.1
µin/in-°F <br>@Temperature -22.0 - 86.0 °F
|
|
|
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled
Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications.
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature -30.0 - 30.0 °C
|
16.1
µin/in-°F <br>@Temperature -22.0 - 86.0 °F
|
ASTM D696 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL159 PA 66
LNP* LUBRICOMP* RFL159 is a compound based on Nylon 66 resin containing 25% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant, Flame Retardant
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature -30.0 - 30.0 °C
|
16.1
µin/in-°F <br>@Temperature -22.0 - 86.0 °F
|
ASTM D696 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL449 PA 66
LNP* LUBRICOMP* RFL449 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Flame Retardant.
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature -30.0 - 30.0 °C
|
16.1
µin/in-°F <br>@Temperature -22.0 - 86.0 °F
|
ASTM D696 |
|
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA12
LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature 23.0 - 60.0 °C
|
16.1
µin/in-°F <br>@Temperature 73.4 - 140 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Europe-Africa-Middle East)
LNP* LUBRICOMP* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features include: Flame Retardant, Internally Lubricated.
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature 23.0 - 60.0 °C
|
16.1
µin/in-°F <br>@Temperature 73.4 - 140 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics LNP STAT-KON RX98063 PA 66 (Europe-Africa-Middle East)
LNP* STAT-KON* RX98063 is a compound based on PA 66 resin containing Glass Fiber, Stainless Steel Fiber. Added features include; Antistatic.
|
|||
| CTE, linear, Parallel to Flow |
28.9
µm/m-°C <br>@Temperature -30.0 - 30.0 °C
|
16.1
µin/in-°F <br>@Temperature -22.0 - 86.0 °F
|
ASTM D696 |
|
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC
LNP* Thermocomp* DF004RXP is a compound based on Polycarbonate resin containing 20% Glass Fiber. Some light color grades may have lower impact data than natural and black. Added features include: ..
|
|||
| CTE, linear, Parallel to Flow |
28.9
µm/m-°C <br>@Temperature -30.0 - 30.0 °C
|
16.1
µin/in-°F <br>@Temperature -22.0 - 86.0 °F
|
ASTM D696 |
|
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC (Asia Pacific)
20% Glass Fiber Reinforced Polycarbonate. Some light color grades may have lower impact data than nature and black grade.
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature -30.0 - 30.0 °C
|
16.1
µin/in-°F <br>@Temperature -22.0 - 86.0 °F
|
ASTM D696 |
|
SABIC Innovative Plastics LNP THERMOCOMP EX93452 PEI
LNP THERMOCOMP* EX93452 is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Electrically Conductive.
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature -30.0 - 30.0 °C
|
16.1
µin/in-°F <br>@Temperature -22.0 - 86.0 °F
|
ASTM D696 |
|
SABIC Innovative Plastics LNP THERMOCOMP PDXE98480 PEI
LNP* Thermocomp* PDXE98480 is a compound based on Polyetherimide with Proprietary Fillers. Added feature of this grade: Reinforced.
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature 23.0 - 60.0 °C
|
16.1
µin/in-°F <br>@Temperature 73.4 - 140 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics LNP THERMOCOMP PFB55 PA 6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* PFB55 is a compound based on PA 6 resin containing Glass Bead, Glass Fiber.
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature 23.0 - 60.0 °C
|
16.1
µin/in-°F <br>@Temperature 73.4 - 140 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics LNP THERMOCOMP ZF006 PPE+PS (Europe-Africa-Middle East)
LNP* THERMOCOMP* ZF006 is a compound based on PPE+PS Blend resin containing Glass Fiber
|
|||
| CTE, linear, Parallel to Flow |
28.9
µm/m-°C <br>@Temperature -40.0 - 40.0 °C
|
16.1
µin/in-°F <br>@Temperature -40.0 - 104 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics NORYL GFN2 PPE+PS
PPE+PS blend. 20% Glass reinforced. UL746C F1. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional sta..
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature -30.0 - 30.0 °C
|
16.1
µin/in-°F <br>@Temperature -22.0 - 86.0 °F
|
ASTM D696 |
|
SABIC Innovative Plastics LNP STAT-KON FX91304 PE
LNP* STAT-KON* FX91304 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature -30.0 - 30.0 °C
|
16.1
µin/in-°F <br>@Temperature -22.0 - 86.0 °F
|
ASTM D696 |
|
SABIC Innovative Plastics LNP THERMOCOMP EF006E PEI
LNP THERMOCOMP* EF006E is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
|
|||
| CTE, linear, Parallel to Flow | 29.0 µm/m-°C | 16.1 µin/in-°F | ISO 11359-1/-2 |
|
DuPont Performance Polymers Rynite® FR515 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**)
15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8m..
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature 23.0 - 60.0 °C
|
16.1
µin/in-°F <br>@Temperature 73.4 - 140 °F
|
ISO 11359-2 |
|
Eurostar Staramide BG6ST43 PA6, 30% Glass Fiber Filled, Impact Modified, Injection Molded
BG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature 20.0 °C
|
16.1
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Covestro Bayblend® KL 1-1427 Polycarbonate/ABS Blend
Glass fiber reinforced grade (30%) with high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – ..
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature 20.0 °C
|
16.1
µin/in-°F <br>@Temperature 68.0 °F
|
ASTM E831 |
|
Sumitomo Bakelite North America FM 4005X4649 Fiberglass Reinforced Phenolic Novolac
FM 4005X4649 a fiberglass reinforced two-step phenolic molding compound formulated to increase thermal conductivity, to provide static dissipation and good wear resistance to abrasive media.Informat..
|
|||
| CTE, linear, Parallel to Flow |
29.0
µm/m-°C <br>@Temperature 20.0 °C
|
16.1
µin/in-°F <br>@Temperature 68.0 °F
|
ASTM D696 |
|
Sumitomo Bakelite North America RX® 1-510N Mineral Filled Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ..
|
|||
| CTE, linear, Parallel to Flow | 29.0 µm/m-°C | 16.1 µin/in-°F | ISO 11359-2 |
|
Solvay Specialty Polymers Ixef® 5002 Polyarylamide (PARA), 20% GlassPTFE
(discontinued **)
Ixef 5002 is a 20% glass-fiber reinforced, PTFE modified polyarylamide which exhibits very good mechanical performance, very good surface gloss, and superior wear properties.- Natural: Ixef 5002/008..
|
|||