| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Unnotched |
3.74
J/cm <br>@Thickness 3.18 mm
|
7.01
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
LNP Thermocomp® EC-1006 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
|
|||
| Izod Impact, Unnotched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D4812 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL449 PA 66
LNP* LUBRICOMP* RFL449 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Flame Retardant.
|
|||
| Izod Impact, Unnotched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D4812 |
|
SABIC Innovative Plastics LNP THERMOCOMP AF004XXY ABS
LNP* Thermocomp* AF004XXY is a compound based on ABS containing 20% glass fiber.
|
|||
| Izod Impact, Unnotched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D4812 |
|
SABIC Innovative Plastics LNP THERMOCOMP AX02749 ABS
LNP* THERMOCOMP* AX02749 is a compound based on ABS containing proprietary fillers.
|
|||
| Izod Impact, Unnotched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D4812 |
|
SABIC Innovative Plastics LNP THERMOCOMP KB006 Acetal
LNP* THERMOCOMP* KB006 is a compound based on Acetal containing 30% Glass Bead.
|
|||
| Izod Impact, Unnotched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D4812 |
|
SABIC Innovative Plastics LNP STAT-KON KE002 ACETAL
LNP* STAT-KON* KE002 is a compound based on Acetal resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.
|
|||
| Izod Impact, Unnotched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
|
A. Schulman ComAlloy Comtuf® 639 Nylon 6/6, Mineral Reinforced, Impact Modified, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.40% Mineral reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i..
|
|||
| Izod Impact, Unnotched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
|
A. Schulman ComAlloy Hiloy® 754 Glass Reinforced, Flow Enhanced, PPS Alloy, UL
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Izod Impact, Unnotched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
|
A. Schulman ComAlloy Voloy® 417 Polyester - PBT, Glass/Mineral Reinforced, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.43% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Izod Impact, Unnotched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
|
A. Schulman ComAlloy Hiloy® 518 Polycarbonate, Carbon Fiber Reinforced
Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Izod Impact, Unnotched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
|
A. Schulman ComAlloy Hiloy® 638 Nylon 6/6, Mineral Reinforced, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.35% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Izod Impact, Unnotched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
|
A. Schulman ComAlloy Lubrilon® 628 Nylon 6/6, Glass Fiber/Molybdenum Disulfide Filled, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
|
|||