Physical Properties Metric English Comments
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792A
Resinoid 7051 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792
Quantum Composites QC-2130 Phenolic 25% Glass Fiber SMC  (discontinued **)
QC-2130 is a glass-reinforced sheet molding compound based on a phenolic resin matrix. It exhibits outstanding low flammability characteristics. QC-2130 is recommended for applications such as air..
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide Compound  (Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® BR42B is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surf..
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792
Chevron Phillips Ryton® BR42C Polyphenylene Sulfide Compound  (discontinued **)
Black Polyphenylene Sulfide CompoundRyton® BR42C is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surface fric..
Density 1.75 g/cc
0.0632 lb/in³
ASTM D572
Haysite 270FRII Polyester BMC, Glass Reinforced
Haysite Grade 270FRII is a second generation glass reinforced thermoset polyester bulk molding compound. This material can be compression, transfer, or injection molded. Qualified under MIL-M-14, Ty..
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP KFL36 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KFL36 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Density 1.75 g/cc
0.0632 lb/in³
ISO 1183
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA), 60% Glass Fiber
Amodel® A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional ..
Density 1.75 - 1.80 g/cc
0.0632 - 0.0650 lb/in³
ASTM D792
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)
Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: MembranesAddition..
Density 1.75 - 1.80 g/cc
0.0632 - 0.0650 lb/in³
ASTM D792
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Density 1.75 - 1.78 g/cc
0.0632 - 0.0643 lb/in³
ISO 1183
Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF)
Solef® 5130 PVDF is an ultra high viscosity grade that gives the best adhesion ideal for its usage in lithium batteries.Features: Good Adhesion; Ultra High ViscosityUses: Batteries; BinderAdditio..
Density 1.75 - 1.80 g/cc
0.0632 - 0.0650 lb/in³
ASTM D792
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)
Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran..
Density 1.75 g/cc
0.0632 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp 5C004
LNP* Thermocomp* 5C004 is a compound based on Polyvinylidene Fluoride resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC..
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP 5C004 FP-V (PVDF)
LNP* THERMOCOMP* 5C004 is a compound based on Polyvinylidene Fluoride resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792
Sumitomo Bakelite North America 51-01 CAFR-P Mineral Filled Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ..
Density 1.75 g/cc
0.0632 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp 2C004
LNP THERMOCOMP* 2C004 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup..
Density 1.75 g/cc
0.0632 lb/in³
ISO 1183
Polyplastics Duranex® CN7130 Polybutylene Terephthalate (PBT), Low friction, Low wear, GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792
Tipco Tipcolite® THD 411 Phenolic Compound, Mica, Asbestos & Cellulose, Medium Flow & High Electrical Properties
Medium Flow Phenolic Compound, Reinforced with Mica, Asbestos & CelluloseApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr..
Density 1.75 g/cc
0.0632 lb/in³
Toho Tenax Besfight® G30-500 12K HTA-7C NS01 Continuous Filament Carbon Fiber
Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car..
Density 1.75 g/cc
0.0632 lb/in³
Toho Tenax Besfight® G30-500 3K HTA-7C EP03 Continuous Filament Carbon Fiber
Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car..
Density 1.75 g/cc
0.0632 lb/in³
Zoltek Panex 30® High Twist Carbon Roving
High Twist Carbon RovingApplications include: Friction Clutches & Brakes, Composite Substructures
Density 1.75 g/cc
0.0632 lb/in³
Zoltek Panex 35® Milled Carbon Fibers
Milled Carbon FibersApplications include: Buoyancy, RFI/EMI Shielding, Static Dissipation, Surface Reinforcement, Low Cost Polyurethane Friction Compounds
Density 1.75 g/cc

@Thickness >=0.000 mm
0.0632 lb/in³

@Thickness >=0.000 in
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 61212-2 7.3
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes
Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength. Retains electrical properties at high air humidity. High resistance to chemicals.Applications..
Density 1.75 - 1.79 g/cc
0.0632 - 0.0647 lb/in³
ISO R 1183
Fainplast Compounds CR 85 Flexible PVC, Electrical Bedding
Bedding
Density 1.75 g/cc
0.0632 lb/in³
ISO 1183
Eurotec® Tecomid® NT40 GR60 NL HS PPA, 60% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792 Method A
Arlon 49N Multifunctional Epoxy Low-Flow Prepreg
49N is a low-flow epoxy prepreg engineered for bonding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. With a high Tg, the prepreg can be used in high-performance or high-te..
Density 1.75 g/cc
0.0632 lb/in³
ISO 1183
BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Dry)
Description: Ultramid HMG14 HS BK-102 is a 60% glass reinforced, injection molding grade of PA66 offering high strength and stiffness. Due to inherently lower moisture absorption, Ultramid HMG14 HS ..
Density 1.75 g/cc
0.0632 lb/in³
A. Schulman ComAlloy E-16902N PPS Alloy, Electrically Conductive - Stainless Steel Fiber Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE
LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s).
Density 1.75 - 1.85 g/cc
0.0632 - 0.0668 lb/in³
ASTM D792