Polyram PlusTek PA600 Nylon 6.6, Heat Stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized
Manufacturer Polyram
Trade Name PlusTek
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PA600 Nylon 6.6, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
DIN 53479
Water Absorption 8.5 %
8.5 %
DIN 53495
Moisture Absorption at Equilibrium 2.8 %
2.8 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.011 - 0.018 cm/cm
0.011 - 0.018 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM-D785
Tensile Strength, Yield 85.0 MPa
12300 psi
ASTM-D638
Elongation at Break 10 %
10 %
ASTM-D638
Flexural Strength 115 MPa
16700 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM-D790
Izod Impact, Notched 0.600 J/cm

@Temperature 23.0 °C
1.12 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
Maximum Service Temperature, Air 115 °C
239 °F
Continuous Use
>= 180 °C
>= 356 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
DIN 53461
Flammability, UL94 V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
DIN 53482
Dielectric Constant 3.3

@Frequency 1e+6 Hz
3.3

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 120 kV/mm
3050 kV/in
VDE 0303/4