Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.010 - 0.018 cm/cm | 0.010 - 0.018 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 RV0 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, halogen and phosphorus free.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.010 - 0.018 cm/cm | 0.010 - 0.018 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 HS-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC 12000 Polypropylene Copolymer Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.012 - 0.018 cm/cm | 0.012 - 0.018 in/in | ASTM D955 |
Polymer Resources NY66-MD02-[color]-H Nylon, 2% Molybdenum disulfide for lubrication and wear, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.013 - 0.018 cm/cm | 0.013 - 0.018 in/in | ASTM D955 |
Polymer Resources PC/TP-GP3 PC/Polyester Alloy High Impact, Superior Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 W-KV10 Nylon 6 for injection molding, 10% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0080 - 0.018 cm/cm | 0.0080 - 0.018 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 W-KV30 Nylon 6 for injection molding, 30% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | |
Lehmann & Voss LUVOCOM® 1850-7692 PBT, with glass spheres and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Linear Mold Shrinkage | 0.010 - 0.018 cm/cm | 0.010 - 0.018 in/in | |
Lehmann & Voss LUVOCOM® 19-7810 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Linear Mold Shrinkage | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | |
Lehmann & Voss LUVOCOM® 19-8074 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Linear Mold Shrinkage | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | |
Polyram PlusTek PA600 Nylon 6.6, Heat Stabilized Heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | |
Polyram PlusTek PA604 Nylon 6.6, Heat Stabilized High heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | |
Polyram PlusTek PA810 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0060 - 0.018 cm/cm @Thickness 3.20 mm |
0.0060 - 0.018 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and .. |
|||
Linear Mold Shrinkage | 0.0060 - 0.018 cm/cm @Thickness 3.20 mm |
0.0060 - 0.018 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit.. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | |
Polyram PlusTek RB133 Nylon 6, General Purpose General purpose polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | ISO DIS 294-4 |
Wellman Wellamid® FR22F-NBK3 Flame Retardant Nylon 66 Description: Flame Retardant Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage | 0.0060 - 0.018 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.0060 - 0.018 in/in @Thickness 0.126 in, Time 72.0 hour |
ISO 294 |
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.018 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.0060 - 0.018 in/in @Thickness 0.126 in, Time 72.0 hour |
ISO 294 |
A. Schulman FORMION™ FI 120 Non-Reinforced, Injection Molding Grade Zinc Ionomer DescriptionFormion® FI 120 is a non-reinforced, transparent, injection molding grade Zinc Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and lo.. |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | |
Polyram PlusTek RA102 Nylon 6.6, General Purpose General purpose polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | ASTM D955 |
Asia International Enterprise (Hong Kong) 3010F Polybutylene terephthalate Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC 15000 Polypropylene Copolymer Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.018 cm/cm | 0.010 - 0.018 in/in | ASTM D955 |
Asia International Enterprise (Hong Kong) ST6010 Nylon 66 Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | after bake; ISO 294 |
Solvay Engineered Polymers DEXPRO® R120 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R120 is a reactor-grade thermoplastic elastomeric olefin resin with a good balance of impact performance, stiffness, and paintability. Applications: Painted bumper fasciasInfor.. |
|||
Linear Mold Shrinkage | 0.013 - 0.018 cm/cm | 0.013 - 0.018 in/in | ASTM D955 |
Polymer Resources PC/TP-GP3 PC Polyester, High Impact, Superior Chemical Resistance
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |