Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
Moisture Absorption | 0.600 % @Temperature 23.0 °C |
0.600 % @Temperature 73.4 °F |
50% RH; ISO 62 |
Water Absorption at Saturation | 5.0 % @Temperature 23.0 °C |
5.0 % @Temperature 73.4 °F |
ISO 62-1 |
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | on Tensile Bar; E2P method |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell R | 118 | 118 | ISO 2039-2 |
Hardness, H358/30 | 145 MPa | 21000 psi | ISO 2039-1 |
Tensile Strength at Break | 70.0 MPa | 10200 psi | 5 mm/min; ISO 527 |
Elongation at Break | 2.0 % | 2.0 % | 5 mm/min; ISO 527 |
Tensile Modulus | 8.00 GPa | 1160 ksi | 1 mm/min; ISO 527 |
Flexural Strength | 110 MPa | 16000 psi | 2 mm/min; ISO 178 |
Flexural Modulus | 7.50 GPa | 1090 ksi | 2 mm/min; ISO 178 |
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
3.00 kJ/m² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A | |
3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1A | |
3.00 kJ/m² @Temperature -40.0 °C |
1.43 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A | |
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1U |
22.0 kJ/m² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1U | |
Charpy Impact Unnotched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU | |
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 179/1eA |
0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eA | |
Taber Abrasion, mg/1000 Cycles | 49 @Load 1.00 kg |
49 @Load 2.20 lb |
CS-17; E2P Method |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
19.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ISO 8302 |
Hot Ball Pressure Test | 123 - 127 °C | 253 - 261 °F | IEC 60695-10-2 |
Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
Deflection Temperature at 1.8 MPa (264 psi) | 170 °C | 338 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Ae |
Vicat Softening Point | 235 °C | 455 °F | B/120; ISO 306 |
237 °C | 459 °F | B/50; ISO 306 | |
Flammability, UL94 | 2.00 @Thickness 0.750 mm |
2.00 @Thickness 0.0295 in |
|
V-1 @Thickness 3.00 mm |
V-1 @Thickness 0.118 in |
||
Oxygen Index | 32 % | 32 % | ISO 4589 |
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
Surface Resistance | >= 1.00e+16 ohm | >= 1.00e+16 ohm | IEC 60093 |
Dielectric Constant | 3.2 @Frequency 1.00e+6 Hz |
3.2 @Frequency 1.00e+6 Hz |
IEC 60250 |
3.4 @Frequency 50.0 - 60.0 Hz |
3.4 @Frequency 50.0 - 60.0 Hz |
IEC 60250 | |
Dielectric Strength | 24.0 kV/mm @Thickness 3.20 mm |
610 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
Dissipation Factor | 0.0104 @Frequency 50.0 - 60.0 Hz |
0.0104 @Frequency 50.0 - 60.0 Hz |
IEC 60250 |
0.0122 @Frequency 1.00e+6 Hz |
0.0122 @Frequency 1.00e+6 Hz |
IEC 60250 | |
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
600 V | 600 V | M; IEC 60112 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Zone 3 | 270 - 285 °C | 518 - 545 °F | |
Melt Temperature | 270 - 285 °C | 518 - 545 °F | |
Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Moisture Content | 0.20 % | 0.20 % |