Material Notes:
Conductive Adhesive Nickel-Plated FabricDescription: CHO-FAB® tape is a corrosion resistant nickel-plated cloth coated with Chomerics’ highly conductive pressure-sensitive adhesive. CHO-FAB® tape is extremely strong and lightweight, and has excellent conformability/wrapability to enhance shielding performance and appearance. Use of corrosion resistant nickel-plated cloth and Chomerics’ superior metal-particle-filled conductive adhesive technology produces a tape used in a wide variety of EMI shielding and grounding applications. Typical Applications: Provide a low impedance connection between a braided cable shield and the metal connector backshell in molded cables. An effective EMI shielded assembly can be achieved without soldering the tape to the braid or backshell; EMI radiation measurement troubleshooting, using CHO-FOIL tape to shield ventilation slots or seam gaps; Provide electrical continuity in seams of EMI shielded rooms and electronic enclosures; Supply electrical contact to surfaces that can’t be soldered to, such as conductive plastic or aluminum; EMI shield for cables by wrapping the tape around the cable. An overlap is recommended; ESD shielding; Provide corrosion-resistant ground contact points; Fabric tape available where weight and flexibility are important, such as for wrapping cables. Information provided by Chomerics
Physical Properties Metric English Comments
Thickness 38.1 microns
1.50 mil
Adhesive thickness
127 microns
5.00 mil
Fabric thickness
165 microns
6.50 mil
Total
Mechanical Properties Metric English Comments
Peel Strength 0.491 kN/m
2.80 pli
Initial; ASTM D1000
0.508 kN/m
<br>@Temperature 85.0 °C
2.90 pli
<br>@Temperature 185 °F
95% RH; ASTM D1000
0.473 kN/m
<br>@Temperature 121 °C,<br> Time 605000 sec
2.70 pli
<br>@Temperature 250 °F,<br> Time 168 hour
ASTM D1000
0.649 kN/m
<br>@Temperature 85.0 °C,<br> Time 605000 sec
3.70 pli
<br>@Temperature 185 °F,<br> Time 168 hour
ASTM D1000
0.368 kN/m
<br>@Time 605000 sec
2.10 pli
<br>@Time 168 hour
Salt fog corrosion; ASTM D1000
Taber Abrasion, mg/1000 Cycles <= 175
<= 175
500 gramweight. CS-10 wheel, 500 cycles; CHO-TP-57
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Surface Resistance <= 0.10 ohm
<= 0.10 ohm
Initial Surface Resistivity (SR); CHO-TP-57
<= 0.10 ohm
<= 0.10 ohm
Initial through resistivity (TR); CHO-TP-57
<= 0.10 ohm
<= 0.10 ohm
Initial Taber Abrasion; CHO-TP-57
<= 0.10 ohm
<br>@Temperature 85.0 °C
<= 0.10 ohm
<br>@Temperature 185 °F
95% RH; (SR); CHO-TP-57
<= 0.15 ohm
<br>@Temperature 85.0 °C
<= 0.15 ohm
<br>@Temperature 185 °F
95% RH; (TR); CHO-TP-57
<= 0.10 ohm
<br>@Temperature 85.0 °C,<br> Time 605000 sec
<= 0.10 ohm
<br>@Temperature 185 °F,<br> Time 168 hour
(SR); CHO-TP-57
<= 0.10 ohm
<br>@Temperature 121 °C,<br> Time 605000 sec
<= 0.10 ohm
<br>@Temperature 250 °F,<br> Time 168 hour
(SR); CHO-TP-57
<= 0.15 ohm
<br>@Temperature 121 °C,<br> Time 605000 sec
<= 0.15 ohm
<br>@Temperature 250 °F,<br> Time 168 hour
(TR); CHO-TP-57
<= 0.15 ohm
<br>@Temperature 85.0 °C,<br> Time 605000 sec
<= 0.15 ohm
<br>@Temperature 185 °F,<br> Time 168 hour
(TR); CHO-TP-57
<= 0.10 ohm
<br>@Time 605000 sec
<= 0.10 ohm
<br>@Time 168 hour
Salt fog corrosion; (SR); CHO-TP-57
<= 1.0 ohm
<br>@Time 605000 sec
<= 1.0 ohm
<br>@Time 168 hour
Salt fog corrosion; (TR); CHO-TP-57
Surface Resistivity per Square <= 0.10 ohm
<= 0.10 ohm
[ohm/in&lt;sup&gt;2&lt;sup&gt;]; &lt;.016 ohm/cm&lt;sup&gt;2&lt;/sup&gt;; MIL-STD-202C
Descriptive Properties Value Comments
Adhesion to Aluminum >40 oz./inch
ASTM D1000
Adhesive Type Electrically Conductive, Pressure-Sensitive Acrylic
Foil/Fabric Type Nickel-Plated Fabric