| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | ASTM D648 |
|
Polymer Resources NY66-M40-[color]-H Nylon 66, 40% Mineral Filled, Heat Stabilized
Nylon 66, 40% Mineral Filled, Lubricated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon ..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | ASTM D648 |
|
Polymer Resources NY6-G43 Nylon 6, 43% Glass Reinforced
Nylon 6, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | Unannealed; ASTM D648 |
|
Ravago Manufacturing Americas Hylon® N1000HL Nylon 6/6
Available in North America Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and Lubricated RoHS Compliant Auto Specifications: FORD WSK-M4D648-A Color: Black Form: Pellets Processi..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | Unannealed; ASTM D648 |
|
Ravago Manufacturing Americas Hylon® N1040MHL Nylon 6/6 (DAM)
Information provided by Ravago.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | ISO 75-1/-2 |
|
DuPont Performance Polymers Rynite® FR515 BK507 PET
(Unverified Data**)
Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | 0.125 in; ASTM D648 |
|
Matrixx Group 85S7451 Flame Retardant 45% Glass Reinforced PET
(discontinued **)
Data provided by The Matrixx Group, formerly RePlas.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | 0.125 in; ASTM D648 |
|
Matrixx Group 80S7451 45% Glass Reinforced PET
(discontinued **)
Data provided by The Matrixx Group, formerly RePlas.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | ASTM D648 |
|
Polymer Resources NY66-M40-[color]H Nylon, 40% Mineral Filled, Lubricated, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | ASTM D648 |
|
Polymer Resources NY6-G43-[color]-H Nylon 6, 43% Glass Reinforced, Heat Stabilized
Nylon 6, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | Unannealed; ASTM D648 |
|
Ravago Manufacturing Americas Hylon® N1000 Nylon 6/6 (DAM)
(discontinued **)
Information provided by Ravago.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | Unannealed; ASTM D648 |
|
Ravago Manufacturing Americas Hylon® N1000EHL Nylon 6/6 (DAM)
(discontinued **)
Information provided by Ravago.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | Unannealed; ASTM D648 |
|
Ravago Manufacturing Americas Hylon® N1000EL Nylon 6/6 (DAM)
(discontinued **)
Information provided by Ravago
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | Unannealed; ASTM D648 |
|
Ravago Manufacturing Americas Hylon® N1200HL BK Nylon 6/6
(discontinued **)
Available in North AmericaAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedAuto Specifications: DELPHI QMPL-1257 Color: BlackForm: PelletsInformation provided by Rava..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 - 280 °C | 460 - 536 °F | Average value: 263 °C Grade Count:9 |
|
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
|
SABIC Innovative Plastics LNP Thermocomp 9X06477 SPS
LNP* Thermocomp* 9X06477 is a compound based on Syndiotactic Polystyrene resin containing Glass Fiber. Characteristics of this grade is Heat Stabilized.This data was supplied by SABIC-IP for the Am..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | ASTM D648 |
|
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | ASTM D648 |
|
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | ASTM D648 |
|
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | ASTM D648 |
|
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | ASTM D648 |
|
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | ASTM D648 |
|
Cheng Yu Plastic N6G30 Nylon 6, 30% Glass Filled |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
|
Eurostar Starflam AFR682B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding
Starflam AFR682B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | ASTM D648 |
|
Adell AR-33 Nylon 66, 15% Glass Reinforced
Data provided by Adell Plastics, Inc.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | ASTM D648 |
|
Adell AJ-34 Nylon 66, 20% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | ASTM D648 |
|
Mitsui AURUM® PL450C Polyimide
(discontinued **)
AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | ISO 75-1/-2 |
|
DuPont Performance Polymers Rynite® RE5264 NC010 PET
(Unverified Data**)
Rynite® RE5264 NC010 is a 36% glass fiber reinforced, color stabilized, modified polyethylene terephthalate.Information provided by DuPont Performance Polymers
|
|||