Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chesterton 613 Moly Grease

Category Fluid , Lubricant
Manufacturer Chesterton
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chesterton 613 Moly Grease.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Chesterton® 613 Moly Grease is a high-performance, cost-effective lubricant that can withstand extreme temperatures and pressures for a wide range of high and low-speed applications. Fortified with molybdenum disulfide, it can handle the toughest of lubricating jobs and last significantly longer than conventional greases. Wear, galling or seizing of greased surfaces can occur even when using high-performance greases, especially when heavy pressures squeeze the grease out of lubricating film. During these extreme pressure conditions, the molybdenum disulfide particles in 613 Moly Grease are left behind on the surface in a thin, adherent, lubricating film. The unique, plate-like geometry of the particles ensures that parts glide smoothly over each other, preventing wear, galling and eventual seizing. Until further applications of the grease can be applied. The product has excellent resistance to water washout, a condition that plagues and shortens the life of many conventional greases and necessitates constant re-lubrication. Since 613 Moly Grease ensures continuous, longer-lasting lubrication and protection, fewer applications are required. Less applications means less maintenance costs and less production downtime. The product’s superior mechanical stability assures that it will not break down or thin out and thus not leak out of the bearings under sustained heavy workloads. Features:Molybdenum disulfide for added boost under extreme conditionsExcellent mechanical stabilityCorrosion inhibitors protect lubricated equipmentExcellent resistance to water washoutSpecial additives for longer life, continuous lubrication.Benefits:Reduce labor, maintenance costsReduce number of reapplications; low product costsSave the cost of replacement partsProlong the life of machinery and partsApplications: 613 Moly Grease lubricates all types of equipment in a wide range of applications that require a high-quality, long-lasting, cost-effective grease. It is especially effective on equipment subjected to extreme pressures during startup, shutdown or in operation. Use 613 Moly Grease for manufacturing and processing equipmentConveyorsMining equipmentPlain and anti-friction bearingsSmall, exposed greatsCams, guides, ways, slidesPress fittings and couplingsElectric motorsFans, blowersPumps, generatorsPresses, shears, hinges.Information provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
Particle Size 0.75 µm
0.75 µm
Molybdenum disulfide
Mechanical Properties Metric English Comments
Four Ball Wear 0.350 mm

@Temperature 54.0 °C,
Time 3600 sec
0.0138 in

@Temperature 129 °F,
Time 1.00 hour
1800 rpm, 20 kg, scar diameter
Penetration 288 - 299
288 - 299
ASTM D217
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 138 °C
280 °F
Minimum Service Temperature, Air -18.0 °C
-0.400 °F
Dropping Point 199 °C
390 °F
ASTM D566
Descriptive Properties Value Comments
Oxidation Stability 0.35 kg/cm2
100 hrs, ASTM D942 pressure drop
1.19 kg/cm2
500 hrs, ASTM D942 pressure drop
Users viewing this material also viewed the following: