Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® MP 90 C High Density Polyethylene - Injection Molding Eraclene MP 90 C is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution and a high .. |
|||
Melt Flow | 7.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
7.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
SABIC FI0750 Bimodal High Density Polyethylene for Blown Film Product Description: FI0750 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Melt Flow | 7.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Network Polymers SAN 277 Blue Tint Color Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Melt Flow | 7.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Network Polymers SAN 278 Medium Blue Tint Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Melt Flow | 7.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Network Polymers SAN 279 Water White Color Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Melt Flow | 7.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® EXL4019 PC (Europe-Africa-Middle East) Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
Melt Flow | 7.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
7.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) BL8 HM 7745 High Density Polyethylene BL8 (HM 7745) is a high density polyethylene with Butene-1 as comonomer.Applications: for heating oil storage tanks, large containers for various chemicals.Information provided by Iran Petrochemical.. |
|||
Melt Flow | 7.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
7.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 4HS HM 9455 F1 High Density Polyethylene EX 4HS is a high density polyethylene with 1-Butene as co monomer. It has high rigidity, low gel level, high drawdown, very high stiffness and good tenacity.Applications: film extrusion, blending .. |
|||
Melt Flow | 7.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
7.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl MX5569 PPE+PS PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-.. |
|||
Melt Flow | 7.5 g/10 min @Load 2.16 kg, Temperature 220 °C |
7.5 g/10 min @Load 4.76 lb, Temperature 428 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Melt Flow | 7.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 3001MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 7.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 3002MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 7.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 3300 Description: General Purpose Utility BlackInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 7.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 3501 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 7.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 3501 Natural 1050 Description: Natural, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 7.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 3502 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 7.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS/PC FC-30 Description: Injection Molding Grade, High Impact, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 7.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers SAN 260 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |