| Category | Polymer , Thermoplastic , ABS Polymer |
| Manufacturer | Clariant |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Clariant Renol ABS3460 ABS, General Purpose, Low Gloss.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0050 cm/cm | 0.0050 in/in | ASTM D955 |
| Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 46.9 MPa | 6800 psi | ASTM D638 |
| Elongation at Yield | 20 % | 20 % | ASTM D638 |
| Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
| Izod Impact, Notched | 1.60 J/cm @Temperature 22.8 °C |
3.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 87.8 °C | 190 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 216 - 249 °C | 420 - 480 °F | |
| Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
| 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial | |
| Back Pressure | 0.345 - 1.72 MPa | 50.0 - 250 psi | |
| Shot Size | 30 - 80 % | 30 - 80 % | |
| Screw Speed | 20 - 100 rpm | 20 - 100 rpm |