Polymer Property : Melt Temperature = 249 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Melt Temperature 221 - 249 °C
430 - 480 °F
PolyOne Stat-Tech™ AS-08CF/000 UV FR V0 Acrylonitrile Butadiene Styrene (ABS)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP 1023 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP 1093L Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP 1249B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-1274G Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-1442A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-1488A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-1538A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-1566L3 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-1709C Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-1846-L3 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-1880 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-1885UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-2024A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-2207 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-2327-R Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-2334-R2 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-1349A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-1353A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-1380A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-2455 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-2860M Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP-4123 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 193 - 249 °C
379 - 480 °F
blow molding
Total PPR 3230XZ Polypropylene, Blow Molding Grade
Homopolymer Blow Molding GradeLubricated – FINA 3230XZ offers superior core road release, eliminating the need for additional lubricant.Antistat – FINA 3230XZ contains antistat to minimize dust ac..
Melt Temperature 191 - 249 °C
375 - 480 °F
Clariant Remafin PESP0006 High Density Polyethylene, 10% Glass Fiber
Data provided by Clariant Masterbatches
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Teknor Apex Monprene® MP 1210A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Temperature 182 - 249 °C
360 - 480 °F
Average value: 223 °C Grade Count:5
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim..
Melt Temperature 227 - 249 °C
440 - 480 °F
Molding
PolyOne Edgetek® PS-20GF/000 FR Polybutylene Terephthalate (PBT), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.