Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
Polymer Resources NY66-IM2-LM Nylon, Preliminary Data Sheet, Low Flexural Modulus, High Impact (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Mold Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
Northstar Polymers MSS-A85C Ester Base Polyurethane This high performance polyester system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane elastomers molded with this system exhibit hig.. |
|||
Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Mold Temperature | 26.7 - 93.3 °C | 80.0 - 200 °F | |
PTS Trimid® N66-SG33-BK 33% Glass Reinforced, High Impact Black Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 26.7 - 93.3 °C | 80.0 - 200 °F | |
PTS Trimid® N66-T100 Toughened Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
PTS Tristar® PC-10R-(VE) 12 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
PTS Tristar® PC-10R-(V) 10 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
PTS Tristar® PC-10R-(V22) 22 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 48.9 - 93.3 °C | 120 - 200 °F | Average value: 71.1 °C Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
LTL Color Compounds ColorFast® PC150 Polycarbonate 15 melt high flow polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 66 PTFE20 HS 20% PTFE Lubricated, Heat Stabilized Nylon 6/6 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
Clariant Renol PA101F/ST801 Nylon 66, Impact Modified, Lubricated Data provided by Clariant Masterbatches |