| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black
Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
Network Polymers F7000 Polystyrene
Description: Ignition RetardantInformation provided by Network Polymers Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
Quadrant EPP Fluorosint® HPV Mica-filled PTFE (ASTM Product Data Sheet) |
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
Polymer Resources ABS-GP1 General Purpose ABS
General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
Polymer Resources NY66-MD02 Nylon, 2% Molybdenum disulfide for lubrication and wear (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
Polymer Resources NY66-MD1 Nylon 66, 1% MoS2
Nylon 66, 1% Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
Polymer Resources PPX-FR1-[color]EN Modified PPO, UL 94 V-0 with HDT of 190 F, Extrusion Grade
Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
Polymer Resources TP-M30 Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced Warpage
Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | Unannealed; ASTM D648 |
|
Ravago Manufacturing Americas Hylon® N1000NL2 Nylon 6/6 (Cond)
Information provided by Ravago.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
RheTech Products HP505-01 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black
Applications: Glove box binConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | Annealed; ASTM D648 |
|
Network Polymers NPS 80-1410 Polystyrene
Description: Injection Molding Grade, Medium Impact, High Melt FlowInformation provided by Network Polymers Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
Quadrant EPP Semitron® CMP LL5 Polyester (ASTM Product Data Sheet)
Enhanced semi-crystalline polyester product for extended service in CMP retaining rings. Superior performance, especially in oxide processes, and cost effective relative to standard ring materials. ..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | Unannealed; ASTM D648 |
|
Techmer ES Plastiblend® ABS 7000
Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | Unannealed; ISO 75-2/A; ASTM D648 |
|
Styron MAGNUMâ„¢ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low ..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | Unannealed; ASTM D648 |
|
Techmer ES HiFill FR® PP CO FR-N
Availability: North AmericaForms: PelletsFeatures: Flame Retardant, High Impact Resistance and CopolymerInformation provided by TP Composites, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | unannealed, .125in; ASTM D648 |
|
Star Plastics ABS3545 Molding Grade ABS
Information provided by Star Plastics, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | Unannealed; ASTM D648 |
|
Chase Plastics CP Pryme® NN100HL (Dry) Nylon 66, Heat Stabilized, Lubricated
Features: Heat StabilizedLubricatedForm: PelletsInformation provided by Chase Plastics.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
Chase Plastics CP Pryme® NN100HSL (COND, 50% RH) Nylon 66, Heat Stabilized, Internally Lubricated
Information provided by Chase Plastics.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content)
DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content)
DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
|
Diamond Polymers ABS 4000HH-ELG
Description: Heat Resistant Grade, Low Gloss, Medium High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
Clariant Renol BR4014BK ABS, High Gloss, Black
Data provided by Clariant Masterbatches
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | |
|
Aclo Accutech Polypropylene Homopolymer HP0336T40L1 Talc Reinforced |
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
Americas Styrenics STYRON® 421 High Impact Polystyrene
Product CharacteristicsStiffness/FlowHeat resistanceContact clarityFood Contact CompliantUL Classification 94HBTypical ApplicationsAppliancesRefrigerationPackaging/disposablesConsumer electronicsInf..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | ASTM D648 |
|
Americas Styrenics STYRON® 666D High Heat Crystal Polystyrene
Product CharacteristicsMedium heat resistanceMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsMedicalPackaging/disposablesInformation provided by AmericasStyrenics LLC.
|
|||