Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® 6501A Blow Molding and Injection Molding Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Blow Molding Grade
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 6501A Blow Molding and Injection Molding Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Impact CopolymerApplications: Blow molded bottles and containers, blown and cast film applications, and profile extrusions such as corrugated board.Formolene 6501A is a medium impact copolymer with an excellent balance of toughness and stiffness. It is suited for blow molded bottles and containers, blown and cast film applications, and profile extrusions.Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.Specimens were injection molded according to the conditions specified in ASTM D4101.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 0.70 g/10 min

@Temperature 230 °C
0.70 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 25.5 MPa
3700 psi
2" (50mm) per min.; ASTM D638
Elongation at Yield 10 %
10 %
2" (50mm) per min.; ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
3.42 J/cm

@Temperature 0.000 °C
6.40 ft-lb/in

@Temperature 32.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648