| Nylene® 204 (HS) , Fast Cycle Nylon 6 |
Nylon 6, Unreinforced |
|
| Nylene® 321 (HS) Impact Modified Nylon 6 |
Nylon 6, Unreinforced |
|
| Nylene® 400 Nylon 6, Extrusion Grade |
Nylon 6, Extruded |
|
| Nylene® 401, Nylon 6 |
Nylon 6, Unreinforced, Flame Retardant |
|
| Nylene® 401, Nylon 6, at 50% Relative Humidity |
Nylon 6, Unreinforced |
|
| Nylene® 401D, Nylon 6 |
Nylon 6, Unreinforced |
|
| Nylene® 402 Nylon 6 |
Nylon 6, Unreinforced |
|
| Nylene® 404 Nylon 6 |
Nylon 6, Heat Stabilized |
|
| Nylene® 404 Nylon 6, 50% RH |
Nylon 6, Heat Stabilized |
|
| Nylene® 406 Nylon 6 |
Nylon 6, Unreinforced, Flame Retardant |
|
| Nylene® 406 Nylon 6, 50% RH |
Nylon 6, Unreinforced |
|
| Nylene® 406F Nylon 6 |
Nylon 6, Unreinforced |
|
| Nylene® 406F Nylon 6, 50% RH |
Nylon 6, Unreinforced |
|
| Nylene® 409 Nylon 6 |
Nylon 6, Heat Stabilized |
|
| Nylene® 409 Nylon 6, 50% RH |
Nylon 6, Heat Stabilized |
|
| Nylene® 4114-14 GL (HS) , 14% Glass Fiber Reinforced, Impact Modified Nylon 6/6 |
Nylon 66, 10% Glass Fiber Filled |
|
| Nylene® 4121 (HS) Low Wear Nylon 6/6 |
Nylon 66, Unreinforced |
|
| Nylene® 4214-15 (HS) , 15% Glass Fiber Reinforced Impact Modified Nylon 6 |
Nylon 6, 20% Glass Fiber Filled |
|
| Nylene® 4214-33 (HS) , 33% Glass Fiber Reinforced Impact Modified Nylon 6 |
Nylon 6, 40% Glass Fiber Filled |
|
| Nylene® 451 Nylon 6 |
Nylon 6, Unreinforced, Flame Retardant |
|
| Nylene® 451 Nylon 6, 50% RH |
Nylon 6, Unreinforced |
|
| Nylene® 452 Nylon 6 |
Nylon 6, Unreinforced |
|
| Nylene® 453 Nylon 6 |
Nylon 6, Unreinforced |
|
| Nylene® 453 Nylon 6, 50% RH |
Nylon 6, Unreinforced |
|
| Nylene® 454 Nylon 6 |
Nylon 6, Heat Stabilized |
|
| Nylene® 454 Nylon 6, 50% RH |
Nylon 6, Heat Stabilized |
|
| Nylene® 5143 MS , 43% Glass Reinforced Low Wear Nylon 6/6 |
Nylon 66, 40% Glass Fiber Filled |
|
| Nylene® 600 Nylon 6 |
Nylon 6, Extruded |
|
| Nylene® 600 Nylon 6, 50% RH, Extrusion Grade |
Nylon 6, Extruded |
|
| Nylene® 601 Nylon 6, 50% RH, Extrusion Grade |
Nylon 6, Extruded |
|
| Nylene® 601 Nylon 6, Extrusion Grade |
Nylon 6, Extruded |
|
| Nylene® 603 Nylon 6, Extrusion Grade |
Nylon 6, Extruded |
|
| Nylene® 607 Nylon 6, 50% RH, Extrusion Grade |
Nylon 6, Extruded |
|
| Nylene® 607 Nylon 6, Extrusion Grade |
Nylon 6, Extruded |
|
| Nylene® 609 Nylon 6, 50% RH, Film/Extrusion Grade |
Nylon 6, Film Grade |
|
| Nylene® 609 Nylon 6, Film/Extrusion Grade |
Nylon 6, Film Grade |
|
| Nylene® 6111 (HS) , 40% Glass/Mineral Reinforced Nylon 6/6 |
Nylon 66, Glass/Mineral Filled |
|
| Nylene® 615 Nylon 6, Film Grade |
Nylon 6, Film Grade |
|
| Nylene® 615I Nylon 6, Film Grade |
Nylon 6, Film Grade |
|
| Nylene® 615SA Nylon 6, Film Grade |
Nylon 6, Film Grade |
|
| Nylene® 7139 (HS) Low Wear Nylon 6/6 |
Nylon 66, Unreinforced |
|
| Nylene® 721 Nylon 6 |
Nylon 6, Impact Grade |
|
| Nylene® 724 Nylon 6 |
Nylon 6, Heat Stabilized |
|
| Nylene® 7250 C HS , 50% Glass Fiber/Ceramic Reinforced, Low Warp, High Stiffness Specialty Nylon |
Nylon |
|
| Nylene® 733 Nylon 6 |
Nylon 6, Impact Grade |
|
| Nylene® 734 Nylon 6 |
Nylon 6, Heat Stabilized |
|
| Nylene® 8100 Unfilled Nylon 6/12 |
Nylon 612, Unreinforced |
|
| Nylene® 826 Nylon Copolymer |
Nylon |
|
| Nylene® 9110 G33 , 33% Glass Reinforced Nylon 6/10 |
Nylon 610, Glass Reinforced |
|
| Nylene® 9110 G43 , 43% Glass Reinforced Nylon 6/10 |
Nylon 610, Glass Reinforced |
|
| Nylene® 9110 Unfilled Nylon 6/10 |
Nylon 610 |
|
| Nylene® 9533 , 33% Glass Reinforced Nylon 6/12 |
Nylon 612, Glass Fiber Filler |
|
| Nylene® 9543 , 43% Glass Reinforced Nylon 6/12 |
Nylon 612, Glass Fiber Filler |
|
| Nylene® 9633 , 33% Glass Reinforced Nylon 6,6/6 |
Nylon 66/6, 40% Glass Fiber Reinforced |
|
| Nylene® 9643 , 43% Glass Reinforced Nylon 6,6/6 |
Nylon 66/Nylon 6 Blend, Glass Fiber Filled |
|
| Nylene® CX3395 Nylon Copolymer |
Nylon |
|
| Nylene® CX3451 Translucent Nylon Copolymer |
Nylon |
|
| Nylene® Mach 6 , Fast Cycle Nylon 6 |
Nylon 6, Unreinforced |
|
| Nylene® Naxel™ A914 Polycarbonate/ABS Alloy |
Polycarbonate/ABS Alloy, Unreinforced |
Naxel™
|
| Nylene® Naxel™ AX190 PPE (Polyphenylene Ether) |
Polyphenylene Ether, Molded |
Naxel™
|
| Nylene® Naxel™ B720 Polycarbonate/PBT Alloy |
Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled |
Naxel™
|
| Nylene® Naxel™ PC10 Polycarbonate |
Polycarbonate, Molded |
Naxel™
|
| Nylene® Naxel™ PC1210 Polycarbonate |
Polycarbonate, Molded |
Naxel™
|
| Nylene® Naxel™ PC30 Polycarbonate |
Polycarbonate, Molded |
Naxel™
|
| Nylene® Naxel™ PC43 UV Resistant Polycarbonate |
Polycarbonate, UV Stabilized |
Naxel™
|
| Nylene® Naxel™ PC45G FR 10% Glass Reinforced, Flame Retardant Polycarbonate |
Polycarbonate, Glass Fiber Filled, Flame Retardant |
Naxel™
|
| Nylene® Naxel™ PC502 10% Glass Reinforced Polycarbonate |
Polycarbonate, 10% Glass Filled |
Naxel™
|
| Nylene® Naxel™ PC504 20% Glass Reinforced Polycarbonate |
Polycarbonate, 20% Glass Filled |
Naxel™
|
| Nylene® Naxel™ PC506 30% Glass Reinforced Polycarbonate |
Polycarbonate, 30% Glass Filled |
Naxel™
|
| Nylene® Naxel™ PC524 Flame Retardant Polycarbonate |
Polycarbonate, Unreinforced, Flame Retardant |
Naxel™
|
| Nylene® Naxel™ PC530-112 UV Resistant Polycarbonate |
Polycarbonate, UV Stabilized |
Naxel™
|
| Nylene® Norpex® AX10GF , 10% Glass Reinforced Polyphenylene Ether |
Polyphenylene Ether, 10% Glass Filled |
Norpex®
|
| Nylene® Norpex® AX200 Impact Modified Polyphenylene Ether |
Polyphenylene Ether, Impact Grade |
Norpex®
|
| Nylene® Norpex® AX20GF , 20% Glass Reinforced Polyphenylene Ether |
Polyphenylene Ether, 20% Glass Filled |
Norpex®
|
| Nylene® Norpex® AX20MR , 20% Mineral Reinforced Polyphenylene Ether |
Polyphenylene Ether, Mineral Filled |
Norpex®
|
| Nylene® Norpex® AX20MRFR , 20% Mineral Reinforced, Flame Retardant Polyphenylene Ether |
Polyphenylene Ether, Mineral Filled |
Norpex®
|
| Nylene® Norpex® AX225 HI PPE (Polyphenylene Ether), High Impact Grade |
Polyphenylene Ether, Impact Grade |
Norpex®
|
| Nylene® Norpex® AX235 PPE (Polyphenylene Ether) |
Polyphenylene Ether, Molded |
Norpex®
|
| Nylene® Norpex® AX245 PPE (Polyphenylene Ether) |
Polyphenylene Ether, Molded |
Norpex®
|
| Nylene® Norpex® AX265 PPE (Polyphenylene Ether) |
Polyphenylene Ether, Molded |
Norpex®
|
| Nylene® Norpex® AX290 PPE (Polyphenylene Ether); High Performance High Heat |
Polyphenylene Ether, Heat Resistant |
Norpex®
|
| Nylene® Norpex® AX300 PPE (Polyphenylene Ether); Premium Performance High Heat |
Polyphenylene Ether, Heat Resistant |
Norpex®
|
| Nylene® Norpex® AX30GF , 30% Glass Reinforced Polyphenylene Ether |
Polyphenylene Ether, 30% Glass Filled |
Norpex®
|
| Nylene® NX1440 Nylon 6 |
Nylon 6, Unreinforced |
|
| Nylene® NX3024 Nylon 6 |
Nylon 6, Unreinforced |
|
| Nylene® NX3055I Nylon 6 |
Nylon 6, Film Grade |
|
| Nylene® NX3411 Nylon 6 |
Nylon 6, Film Grade |
|
| Nylene® NX4301 Nylon 6, Extrusion Grade |
Nylon 6, Extruded |
|
| Nylene® NX4528 Unfilled Nylon 6,6/6 |
Nylon 66/6, Unreinforced |
|
| Nylene® NX4569 Nylon 6 |
Nylon 6, Unreinforced |
|
| Nylene® NX4747 , 14% Glass Reinforced Translucent Nylon |
Nylon |
|
| Nylene® NX5703 Nylon 6, Impact Extrusion Grade |
Nylon 6, Extruded |
|
| Nylene® PA6 Glass Filled 5213 HS Nylon 6 |
Nylon 6, 10% Glass Fiber Filled |
|
| Nylene® PA6 Glass Filled 5233 HS Nylon 6 |
Nylon 6, 40% Glass Fiber Filled |
|
| Nylene® PA6 Glass Filled 5243 HS Nylon 6 |
Nylon 6, 30% Glass Fiber Filled |
|
| Nylene® PA6 Glass Filled 5250 HS Nylon 6 |
Nylon 6, 50% Glass Fiber Filled |
|
| Nylene® PA6 Glass/Mineral Filled 7115 HS Nylon 6 |
Nylon 6, Glass/Mineral Reinforced |
|
| Nylene® PA6 Homopolymer 201 Nylon 6; Low Viscosity Nucleated |
Nylon 6, Unreinforced |
|
| Nylene® PA6 Impact Modified 323 HS Nylon 6 |
Nylon 6, Extruded |
|
| Nylene® PA6 Impact Modified 421 HS Nylon 6 |
Nylon 6, Unreinforced |
|