Nylene® PA6 Impact Modified 421 HS Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Nylene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® PA6 Impact Modified 421 HS Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Dry as molded.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D955
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ASTM D638
Elongation at Break 150 %
150 %
ASTM D638
Flexural Modulus 1.70 GPa
247 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C
135 °F
ASTM D648