Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylene® Naxel™ PC10 Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Nylene®
Trade Name Naxel™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® Naxel™ PC10 Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Naxel™ PC10 is a 9 melt, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Melt Flow 9.0 g/10 min
9.0 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
265 °F
ASTM D648