Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylene® Naxel™ PC502 10% Glass Reinforced Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled
Manufacturer Nylene®
Trade Name Naxel™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® Naxel™ PC502 10% Glass Reinforced Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Naxel™ PC502 is a 10% glass fiber reinforced polycarbonate. PC502 is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Melt Flow 8.0 g/10 min
8.0 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 60.7 MPa
8800 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Modulus 3.03 GPa
440 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
265 °F
ASTM D648
Users viewing this material also viewed the following: