Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylene® 733 Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer Nylene®
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Nylene® 733 Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Dry as molded. Injection molding grade. Nylene 733 is a high impact modified nylon suitable for both molding and extrusion. Parts molded from 733 have excellent impact strength right out of the mold without post conditioning. Highlights of Nylene 733 include high stiffness and high strength. Cylinder temperatures should be in the 500 - 550ºF range.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 72.0 MPa
10400 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 8.40 J/cm
15.7 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °C
142 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Processing Temperature 275 °C
527 °F
Users viewing this material also viewed the following: