Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Nylene®
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Nylene® 406F Nylon 6, 50% RH.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded from 406F have better dimensional stability at moisture equilibrium than parts molded from conventional nylon.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Izod Impact, Notched 2.50 J/cm
4.68 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 182 °C
360 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 232 - 243 °C
450 - 469 °F
At Nozzle
Nozzle Temperature 232 - 243 °C
450 - 469 °F