Nylene® 9110 G33 , 33% Glass Reinforced Nylon 6/10

Category Polymer , Thermoplastic , Nylon , Nylon 610 , Nylon 610, Glass Reinforced
Manufacturer Nylene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® 9110 G33 , 33% Glass Reinforced Nylon 6/10.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Nylene® 9110 G33 is a 33% glass fiber reinforced nylon 6/10. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 145 MPa
21000 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 214 °C
418 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 196 °C
385 °F
ASTM D648