HOME
ABOUT US
PRODUCT
Thermoplastic
Thermoset
Adhesive
RenewableRecycled-Polymer
RenewableRecycled-Film
Tape
RECENT UPDATE
Company News
Product News
CONTACT US
RFQ
POLYMER SEARCH
SEARCH
HOME
POLYMER SEARCH
Lanxess
Lanxess > Nylon 66, 30% Glass Fiber Filled
Manufacturer :
Lanxess
>
Category :
Nylon 66, 30% Glass Fiber Filled
Product List
Tips:
Up to 100 items are displayed.
PRODUCT NO.
Category
Trade Name
Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced
Nylon 66, 30% Glass Fiber Filled
Durethan®
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber
Nylon 66, 30% Glass Fiber Filled
Durethan®
Lanxess Durethan® AKV 30 G HR DUS023 900116 Nylon 66, 30% Glass Fiber
Nylon 66, Heat Stabilized
Durethan®
Lanxess Durethan® AKV 30 GIT H2.0 900116 Nylon 66, 30% Glass Fiber
Nylon 66, 30% Glass Fiber Filled
Durethan®
Lanxess Durethan® AKV 30 H2.0 901510 Nylon 66, 30% Glass Fiber
Nylon 66, 30% Glass Fiber Filled
Durethan®
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers
Nylon 66, 30% Glass Fiber Filled
Durethan®
Lanxess Durethan® AKV 30 HR H2.0 900116 Nylon 66, 30% Glass Fiber
Nylon 66, 30% Glass Fiber Filled
Durethan®
Lanxess Durethan® AKV 30 HR H2.0 901510 Nylon 66, 30% Glass Fiber
Nylon 66, 30% Glass Fiber Filled
Durethan®
Lanxess Durethan® AKV 325 H2.0 901510 Nylon 66, 25% Glass Fiber
Nylon 66, 30% Glass Fiber Filled
Durethan®
Lanxess Durethan® DP 2802/30 000000 Nylon 66, 30% Glass Fiber
Nylon 66, Glass Fiber Filled, Flame Retardant
Durethan®
Lanxess Durethan® DP AKV 30 FN00 000000 Nylon 66, 30% Glass Fiber
Nylon 66, Glass Fiber Filled, Flame Retardant
Durethan®
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber
Nylon 66, 30% Glass Fiber Filled
Durethan®
Lanxess Durethan® DP AKV 30 HR EF 901510 Nylon 66, 30% Glass Fiber
Nylon 66, 30% Glass Fiber Filled
Durethan®
Lanxess Durethan® DP AKV 30 X HR EF 900116 Nylon 66, 30% Glass Fiber
Nylon 66, 30% Glass Fiber Filled
Durethan®
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber
Nylon 66, Glass Fiber Filled, Flame Retardant
Durethan®