Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : BLUESTAR > Category : Thermoplastic Product List

Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
BLUESTAR 101G0 PBT Polybutylene Terephthalate (PBT), Unreinforced, Molded
BLUESTAR 101G20 PBT, 20% Glass Filled Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
BLUESTAR 101G30 PBT, 30% Glass Filled Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
BLUESTAR 201G20 PBT, 20% Glass Filled Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
BLUESTAR 201G25 PBT, 25% Glass Filled Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
BLUESTAR 203G30 PBT, 30% Glass Filled Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
BLUESTAR 403G-MG20 PBT, 20% Glass Filled Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
BLUESTAR 403HF-G20 PBT, 20% Glass Filled Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
BLUESTAR BS025 Acetal Copolymer Acetal Copolymer, Unreinforced
BLUESTAR BS090 Acetal Copolymer Acetal Copolymer, Unreinforced
BLUESTAR BS130 Acetal Copolymer Acetal Copolymer, Unreinforced
BLUESTAR LXS 109 PPE-PS Polystyrene + Polyphenylene Ether, Unreinforced
BLUESTAR LXS 110 PPE-PS Polystyrene + Polyphenylene Ether, Unreinforced
BLUESTAR LXS 312 PPE-HIPS, 20% Mineral Filled Polystyrene + Polyphenylene Ether, Glass + Mineral Filler
BLUESTAR LXS 314 G10 PPE-HIPS, 10% Glass Filled Polystyrene + Polyphenylene Ether, Glass Filler
BLUESTAR LXS 314 G20 PPE-HIPS, 20% Glass Filled Polystyrene + Polyphenylene Ether, Glass Filler
BLUESTAR LXS 314 G30 PPE-HIPS, 30% Glass Filled Polystyrene + Polyphenylene Ether, Glass Filler
BLUESTAR LXS 315 PPE-PS Polystyrene + Polyphenylene Ether, Unreinforced
BLUESTAR PBT 1100 Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
BLUESTAR PBT 1100A Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
BLUESTAR PBT 403M-G30 30% Glass Filled Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
BLUESTAR PBT 6630 30% Glass Filled Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
BLUESTAR 201-G20202 PBT, 20% Glass Filled Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
BLUESTAR 201-G25202 PBT, 25% Glass Filled Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
BLUESTAR 201-G30202 PBT, 30% Glass Filled Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
BLUESTAR 403G-MG30 PBT, 30% Glass Filled Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
BLUESTAR 403HF-G30 PBT, 30% Glass Filled Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
BLUESTAR BS270 Acetal Copolymer Acetal Copolymer, Unreinforced
BLUESTAR LXS 112 PPE-PS Polystyrene + Polyphenylene Ether, Unreinforced
BLUESTAR LXS 115 PPE-PS Polystyrene + Polyphenylene Ether, Unreinforced
BLUESTAR LXS 314 G40 PPE-HIPS, 40% Glass Filled Polystyrene + Polyphenylene Ether, Glass Filler
BLUESTAR PBT 1090 Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
BLUESTAR PBT 403M-G20 20% Glass Filled Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled