Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BLUESTAR 201-G25202 PBT, 25% Glass Filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer BLUESTAR
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF BLUESTAR 201-G25202 PBT, 25% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS).
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.17 %
0.17 %
50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ASTM D955
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 250 °C
20 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ASTM D638
Tensile Modulus 10.0 GPa
1450 ksi
ASTM D638
Flexural Strength 170 MPa
24700 psi
ASTM D790
Flexural Modulus 7.50 GPa
1090 ksi
ASTM D790
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ASTM D256
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 206 °C
403 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Volume Resistivity 1.30e+16 ohm-cm
1.30e+16 ohm-cm
ASTM D257
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149