Polystyrene + Polyphenylene Ether, Glass Filler
Category :
Polystyrene + Polyphenylene Ether, Glass Filler
Product List
Manufacturer
BLUESTAR
Polymer Technology & Services, LLC (PTS)
Polyram
Techmer ES
Tips:
50 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO.
Manufacturer
Trade Name
PTS PPE-LXS 314-10 PPE-HIPS, 10% Glass Filled
Polymer Technology & Services, LLC (PTS)
PTS PPE-LXS 314-20 PPE-HIPS, 20% Glass Filled
Polymer Technology & Services, LLC (PTS)
PTS PPE-LXS 314-30 PPE-HIPS, 30% Glass Filled
Polymer Technology & Services, LLC (PTS)
Polyram RamLloy PN300G2 PPE/PS Alloy, 10% Glass Fiber
Polyram
Polyram RamLloy PN300G4 PPE/PS Alloy, 20% Glass Fiber
Polyram
Polyram RamLloy PN300G6 PPE/PS Alloy, 30% Glass Fiber
Polyram
BLUESTAR LXS 314 G10 PPE-HIPS, 10% Glass Filled
BLUESTAR
BLUESTAR LXS 314 G20 PPE-HIPS, 20% Glass Filled
BLUESTAR
BLUESTAR LXS 314 G30 PPE-HIPS, 30% Glass Filled
BLUESTAR
BLUESTAR LXS 314 G40 PPE-HIPS, 40% Glass Filled
BLUESTAR
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler
Techmer ES HiFill FR® PPO/HIPS GF20 BK 20% Glass Filled
Techmer ES
HiFill FR®