Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 250 - 280 °C | 482 - 536 °F | |
Plastcom PLASTAMID® 6 GF 30 031 TS PA6 reinforced with glass fiber, heat stabilized PA 6 for injection molding, reinforced with 30% glass fiber, heat stabilized, better surface appearance of injection moldings. Decrease in tensile strength by 50 % after 5000 hours at 170°C. Used f.. |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
Plastcom SLOVAMID 66 MI PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |
|||
Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
Polykemi AB POLYblend 45H PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
Polykemi AB POLYblend 65FS GF10 PC/ABS-blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
Polykemi AB POLYblend 65FS PC/ABS-Blend Information provided by Polykemi AB |
|||
Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
Polykemi AB POLYblend 65H MA5 PC/ABS-blend, Low Friction Information provided by Polykemi AB |
|||
Melt Temperature | 245 - 280 °C | 473 - 536 °F | Do not melt above 310°C |
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i.. |
|||
Melt Temperature | 245 - 280 °C | 473 - 536 °F | Do not melt above 310°C |
Nilit Nilamid B3 H G8 40% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G8 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key character.. |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
PolyOne Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66) These products contain flame retardants which are activated by longer residence times in the cylinder and then can decompose. At interruption of the moulding cycle (approx. >5 min) it is recommended.. |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | DAM |
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6
(Unverified Data**) Zytel® 73G30HSL NC010 is a 30% glass fiber reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Melt Temperature | 180 - 280 °C | 356 - 536 °F | Molding |
Ineos Styrenics Avantra® 594E High Impact Styrenic Polymer (NAFTA) Description: Avantra® 594E is a super high-impact polystyrene grade that delivers excellent processing efficiency along with toughness and high gloss in a wide variety of injection molding applic.. |
|||
Melt Temperature | 180 - 280 °C | 356 - 536 °F | Molding |
Ineos Styrenics Polystyrene 476M (NAFTA) High-impact grade of polystyrene with good ESCR designed to provide uniform melt flow for excellent processability.Information provided by BASF.Ineos Styrenics purchased this product line from BASF .. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax BFM30-EL03N1 Nylon 6 30% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax BFM40-DL04N1 Nylon 6 40% Mineral Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | ISO 294 |
Gromax BFG20-FN00N1 Nylon 6 20% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 240 - 280 °C | 464 - 536 °F | Injection Molding |
Styrolution Luran® S 797 S UV White 33999 Q455 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Melt Temperature | 250 - 280 °C | 482 - 536 °F | |
Toyobo GLAMIDE® T-714E Transparent Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
A. Schulman VOLOY™ 462 Hybrid Reinforced PBT Alloy Information provided by A. Schulman. |
|||
Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
Covestro Bayblend® T65 XF Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 120 °Cimproved flowability compared to T65PreprocessingMax. Water content |
|||
Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
Covestro Bayblend® T85 XF Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 130°Cbetter flow than T85PreprocessingMax. Water content |
|||
Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
Covestro Bayblend® T95 MF* Polycarbonate + ABS, Mineral Filled Developmental productInjection molding grade9 % mineral filledvery high heat resistancereduced coefficient of linear thermal expansiontensile modulus = 3350 MPaVicat/B 120 = 142 °CPreprocessingMax... |
|||
Melt Temperature | 250 - 280 °C | 482 - 536 °F | DAM; Injection Molding |
DuPont Performance Polymers Zytel® FN727 BK230A Nylon 6 Zytel® FN727 BK230A is a black, impact modified, plasticizer free, very flexible polyamide 6 alloy resin having good low temperature toughness, good heat aging and good chemical resistance. Uses in.. |
|||
Melt Temperature | 230 - 280 °C | 446 - 536 °F | Coating |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
Toyobo GLAMIDE® T-779 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Melt Temperature | 250 - 280 °C | 482 - 536 °F | |
E-Polymers SEPAZ® LB30 PA6 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Melt Temperature | 250 - 280 °C | 482 - 536 °F | |
Plastcom SLOVASTER® B1 GF 30 PBT, 30% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG45-RN13N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |