Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 210 - 240 °C | 410 - 464 °F | |
Polykemi AB POLYfill PPC T4020 E20 Polypropylene Copolymer, Mineral Reinforced, Modified Information provided by Polykemi AB |
|||
Melt Temperature | 180 - 240 °C | 356 - 464 °F | Recommended |
NOVA Chemicals Novapol® HE-W959-A HDPE Extrusion/Blow Molding Resin HE-W959-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolog.. |
|||
Melt Temperature | 215 - 240 °C | 419 - 464 °F | |
Ineos ABS Lustran® 356 Extrusion, Low-Gloss
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Melt Temperature | 225 - 240 °C | 437 - 464 °F | |
Eastman Tenite 371A-10 Cellulose Acetate Propionate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Melt Temperature | 210 - 240 °C | 410 - 464 °F | |
LATI LATILUB 82-01M Nylon 12 Base, 1% Molybdenum Disulfide Self Lubricating Plastic
(discontinued **) Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Melt Temperature | 210 - 240 °C | 410 - 464 °F | |
LG Chemical EF-378 ABS, Flame Retardant, Halogen Free Information Provided by LG Chem |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical ER451 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Melt Temperature | 210 - 240 °C | 410 - 464 °F | Injection Molding |
LG Chemical HF380XC ABS, High Flow, High Surface Gloss Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres.. |
|||
Melt Temperature | 210 - 240 °C | 410 - 464 °F | Injection Molding |
LG Chemical HI100 ABS, High Impact Feature: Injection Molding, High ImpactApplication: Helmet, Pipe & Fittings, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Temperature | 200 - 240 °C | 392 - 464 °F | Injection Molding |
LG Chemical KEYFLEX BT GN7155F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LG704W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chem.. |
|||
Melt Temperature | 210 - 240 °C | 410 - 464 °F | |
LG Chemical LUPOL TE-5108 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Flow LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
LG Chemical LUPOS GP-2201F General Purpose ABS, 20% Glass Fiber Reinforced, Flame Retardant LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Melt Temperature | 215 - 240 °C | 419 - 464 °F | Extruder |
Ineos ABS Lustran® 256 Extrusion Blending Grade Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi.. |
|||
Melt Temperature | 180 - 240 °C | 356 - 464 °F | |
Lotte Chemical Titan TITANZEX® HF7000 High density polyethylene HF7000 is a high density polyethylene resin for tubular film extrusion. HF7000 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1.. |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 235°C |
Kingfa MAC-451 UV Modified PC/ABS Alloy Features:Excellent balance propertiesGood weather resistanceGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank cov.. |
|||
Melt Temperature | 200 - 240 °C | 392 - 464 °F | |
LATI Latene® 22H2 MX/25 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Special mineral filler. Very good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Melt Temperature | 200 - 240 °C | 392 - 464 °F | |
LATI Latene® EP 22UVH2 MX/25 PP Copolymer, Mineral Reinforced Polypropylene copolymer (PPc) based compound. UV stabilized. Improved thermal stabilization. Special mineral filler. Very good surface appearance. Good elongation.Availability: Africa & Middle East;.. |
|||
Melt Temperature | 200 - 240 °C | 392 - 464 °F | Flat film |
Styrolution Polystyrol 143 E GR 2 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Melt Temperature | 200 - 240 °C | 392 - 464 °F | Flat film |
Styrolution Polystyrol 165 H GR 2 PS Description: Polystyrol 165 H is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.Applications: In blends with high impact Polystyrene or Styrolux; thermo.. |
|||
Melt Temperature | 210 - 240 °C | 410 - 464 °F | Flat film |
Styrolution Polystyrol 168 N GR 2 PS Description: Polystyrol 168 N is a high molecular, heat grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. As blend component with high impact.. |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 210 - 240 °C | 410 - 464 °F | |
Borealis Bormod™ HC905TF Polypropylene Homopolymer for Thermoforming Bormod HC905TF is a low melt flow rate polypropylene homopolymer intended for thermoformed packaging applications. This homopolymer is produced using the Borealis Controlled Crystallinity Polypropy.. |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
Borealis ME6032 Polypropylene ME6032 is a MDPE compound for solid insulation of telephone singles and data cables at high line speed. It contains a metal deactivator. Applications: Dry core and petroleum jelly filled cables. S.. |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
Tisan TISLAMID® 6 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
Tisan TISLAMID® 6 30% Glass Filled Impact Modified, Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
LATI Latimass 53-04 D008 PP Homopolymer, Impact Modified Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Melt Temperature | 210 - 240 °C | 410 - 464 °F | Injection Molding |
LG Chemical SG175G ABS, Super Surface Gloss, High Flow Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |