Processing Properties Metric English Comments
Melt Temperature 220 - 250 °C
428 - 482 °F
Plastcom PLASTALEN® PQ 81 T 10 Polypropylene reinforced with mineral filler
Modified PP for injection molding with the content of 10% mineral filler, impact modified. Delivered in black color.Information Provided by Plastcom spol. s r.o.
Melt Temperature 220 - 250 °C
428 - 482 °F
PolyOne OnForce™ LFT UR-30 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Melt Temperature 220 °C
428 °F
Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene Copolymer, High Slip, Very High Antiblock Version of 7109T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended wit..
Melt Temperature 220 - 245 °C
428 - 473 °F
Start Point: 230°C
Kingfa HIPS-5197 High Impact Polystyrene
Features:UL 94 HB @ 1.6mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientsApplications:Injection moldingGas assistant moldingTV & Audio housingElec..
Melt Temperature 220 - 250 °C
428 - 482 °F
Start Point: 240°C
Kingfa HR-528 Modified ABS
Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd...
Melt Temperature 220 - 240 °C
428 - 464 °F
Start Point: 230°C
Kingfa JE2-R2 ABS/PBT Alloy
Features:Low costExcellent balance propertiesGood processing propertiesGood heat stabilityGood size stabilityGood surfaceApplications:CD-ROM, DVDPrinter, scanner, photocopier cabinetElectric and ele..
Melt Temperature 220 - 250 °C
428 - 482 °F
Injection Molding
LG Chemical LUCON PS4200 ABS+CF
Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Good Dimensional Stability, Low WarpageApplication: IC TrayCAS No. 9003-56-9, 12001-26-2 and 7440-44-0Information provided by LG Ch..
Melt Temperature 220 - 270 °C
428 - 518 °F
Iran Petrochemical (PCC) EX 2 HF 7750 M High Density Polyethylene
EX2 is a high density polyethylene with 1-Butene as co monomer. It has good rigidity and medium molar mass. Applications: monofilaments, ropes, yarns.Information provided by Iran Petrochemical Com..
Melt Temperature 220 - 235 °C
428 - 455 °F
Lavergne VYTEEN ABS 2904 Acrylonitrile Butadiene Styrene
Vyteen ABS 2904 is a black recycled ABS high impact flow terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Excellent resilience -Good proc..
Melt Temperature 220 - 245 °C
428 - 473 °F
Start Point: 230°C
Kingfa FRHIPSV-0 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientApplications:Injection moldingGas assistant moldingTV or aud..
Melt Temperature 220 - 240 °C
428 - 464 °F
LATI Latiblend 5262 PP Homopolymer/PA6
Blend based on Polypropylene homopolymer (PPh) / Polyamide 6 (PA6). Unfilled. High impact resistance. Very good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
Melt Temperature 220 - 270 °C
428 - 518 °F
ISO 294
Styrolution Novodur® E401 ABS
Novodur E401 is a high impact extrusion grade with good surface appearanceInformation provided by Styrolution
Melt Temperature 220 - 260 °C
428 - 500 °F
ISO 294
Styrolution Novodur® H604 ABS
Novodur H604 is a high heat injection molding grade with enhanced chemical resistance, especially suitable for being painted.Information provided by Styrolution
Melt Temperature 220 - 260 °C
428 - 500 °F
ISO 294
Styrolution Novodur® M203FC ABS
Novodur HD M203FC is an injection molding grade especially suitable for medical applications providing high flowability.Information provided by Styrolution
Melt Temperature 220 - 260 °C
428 - 500 °F
ISO 294
Styrolution Terluran® GP-25 ABS
Terluran GP-25 is an easy-flow, general purpose injection molding grade with high resistance to impact and heat distortion; intended for a wide range of applications, particularly in the housings se..
Melt Temperature <= 220 °C
<= 428 °F
Supreme Petrochem SC 6501 Toughened Polystyrene
Characteristics Excellent melt strength Extremely tough Easy printability Easy miscibility with most grades of polystyrene Processing Extrusion Thermoforming Injection MoldingApplications Impac..
Melt Temperature 220 - 250 °C
428 - 482 °F
Sax Polymers SAXALEN PPH335T20 Polypropylene Homopolymer, 20% Talc Filled
SAXALEN PPH335T20 is a 20% mineral filled Polypropylene - Homopolymer intended for injection molding with very good flow properties and higher stiffness by low warpage and good surface appearance.In..
Melt Temperature 220 - 230 °C
428 - 446 °F
Tisan TISESTER® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
Melt Temperature 220 - 240 °C
428 - 464 °F
Tisan TISLAMID® 6 15% Glass Fiber Reinforced Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Melt Temperature 220 - 240 °C
428 - 464 °F
Tisan TISLAMID® 6 30% Glass Filled Impact Modified, Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Melt Temperature 220 - 240 °C
428 - 464 °F
Tisan TISLAMID® 6 Flame Retardant (V0) Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Melt Temperature 220 - 245 °C
428 - 473 °F
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin
ISOPLAST® 101 is an engineering thermoplastic polyurethane resin.Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product li..
Melt Temperature <= 220 °C
<= 428 °F
Total PS CPDS 827 Flame Retardant Polystyrene
POLYSTYRENE (PS) COMPOUND (CPDS) 827 is a high impact flame retardant polystyrene for use in HGW applications. PS CPDS 827 can be supplied in both natural and colored forms.Main Characteristics:DBD..
Melt Temperature 220 °C
428 °F
130 RPM
Equate EMDA-6200 HDPE Blow Molding Resin
EMDA-6200 grade is a high-density polyethylene copolymer resin designed for blow molding small to medium size bottles. It can be used on intermittent as well as continuous blow molding machines for ..
Melt Temperature 220 - 230 °C
428 - 446 °F
E-Polymers SEPAZ® LH50 PP Homopolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Melt Temperature 220 °C
428 °F
Polyram Polytron P50B01 Homopolymer Polypropylene, Chemically Coupled 50% LGF
A chemically coupled 50% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.
Melt Temperature 220 - 260 °C
428 - 500 °F
LATI Latilub 30/R-07GRT PC, Graphite/PTFE Reinforced
Self-lubricating product based on Polystyrene (PS). Graphite / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termo..
Melt Temperature 220 - 260 °C
428 - 500 °F
Borealis Bormod™ HF955MO Polypropylene Homopolymer for Injection Molding
Bormod HF955MO is a high modulus polypropylene homopolymer. Bormod HF955MO is especially developed within the proprietary Borstar technology. The grade utilizes the unique Borstar reactor design c..
Melt Temperature 220 - 280 °C
428 - 536 °F
Premix Thermoplastics PRE-ELEC® PA 1408 Conductive Thermoplastic Compound
PRE-ELEC® PA 1408 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1..