Material Notes:
ME6032 is a MDPE compound for solid insulation of telephone singles and data cables at high line speed. It contains a metal deactivator. Applications: Dry core and petroleum jelly filled cables. Specifications: ASTM D1248 Type II, Class A, Category 5, Grade E4, E5; BS 6234: Type 03; EN 50288; EN 50290-2-23; IEC 60708; ISO 1872-PE, KHN, 27-D003; NF C32-060; and DIN VDE 0207, 2Y11, 2Y12 and 2Y13.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.928 g/cc
0.0335 lb/in³
ISO 1183
Environmental Stress Crack Resistance >= 250 hour

@Temperature 50.0 °C
>= 250 hour

@Temperature 122 °F
Igepal 100%; F20; ASTM D1693-B
Thermal Stress Crack Resistance >= 1.00 hour

@Temperature 105 °C
>= 1.00 hour

@Temperature 221 °F
IEC 60811-4-2/A
Oxidative Induction Time (OIT) 50 min

@Temperature 200 °C
50 min

@Temperature 392 °F
IEC 60811-4-2/B
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
1s; ISO 868
Tensile Strength at Break 17.0 MPa
2470 psi
ISO 527
Elongation at Break 600 %
600 %
ISO 527
Thermal Properties Metric English Comments
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
IEC 60093
Dielectric Constant 2.3

@Frequency 1.00e+6 Hz
2.3

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 22.0 kV/mm

@Frequency 1000 Hz
559 kV/in

@Frequency 1000 Hz
IEC 60250
Dissipation Factor 0.00015

@Frequency 1.00e+6 Hz
0.00015

@Frequency 1.00e+6 Hz
IEC 60250
Processing Properties Metric English Comments
Processing Temperature 70.0 - 100 °C
158 - 212 °F
conductor preheating temperature; 2400 m/min line speed
Middle Barrel Temperature 165 - 230 °C
329 - 446 °F
Melt Temperature 220 - 240 °C
428 - 464 °F
Head Temperature 230 °C
446 °F
Descriptive Properties Value Comments
Petroleum Jelly Absorption (%) 8
IEC 60811-4-2
Copyright © lookpolymers.com All Rights Reserved