| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 220 - 250 °C | 428 - 482 °F | |
|
PolyOne OnForce™ LFT UR-40 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
|
|||
| Melt Temperature | 220 - 230 °C | 428 - 446 °F | |
|
NOVA Chemicals Sclair® 15A Butene HDPE Film Resin
Film Properties. Features: Low gel, good barrier properties, strength and toughness.Applications: Lamination, co-extrusion.Data provided by the manufacturer.
|
|||
| Melt Temperature | 220 °C | 428 °F | |
|
Chevron Phillips 6109CL LLDPE Blown Film Resin, Butene Copolymer
(discontinued **)
Resin Type: Butene Copolymer, High Slip, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE...
|
|||
| Melt Temperature | 220 °C | 428 °F | |
|
Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **)
Resin Type: Hexene Copolymer, High Slip, Very High Antiblock Version of 7109T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended wit..
|
|||
| Melt Temperature | 220 - 250 °C | 428 - 482 °F | Start Point: 240°C |
|
Kingfa HR-528 Modified ABS
Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd...
|
|||
| Melt Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
|
Kingfa JE2-R2 ABS/PBT Alloy
Features:Low costExcellent balance propertiesGood processing propertiesGood heat stabilityGood size stabilityGood surfaceApplications:CD-ROM, DVDPrinter, scanner, photocopier cabinetElectric and ele..
|
|||
| Melt Temperature | 220 - 250 °C | 428 - 482 °F | Start Point: 230°C |
|
Kingfa JH950-602 Low-temperature Resistant & Flame Retardant PC/ABS Alloy
Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surface, high glossApplications:ControllerPlug, socketShell of ammeterSmall hou..
|
|||
| Melt Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
|
Kingfa JH960 6100 Non-halogenated Flame Retardant PC/ABS
Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesChemical resistanceHydrolysis resistanceDrop down resistantSuper high flow ability, suit for thin w..
|
|||
| Melt Temperature | 220 - 250 °C | 428 - 482 °F | Start Point: 245°C |
|
Kingfa MAC-601 DY Modified 60/40 PC/ABS Alloy
Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelPower toolComputer and acce..
|
|||
| Melt Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion Molding |
|
LG Chemical KEYFLEX BT 1072D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Melt Temperature | 220 - 250 °C | 428 - 482 °F | |
|
LG Chemical SH-610 ABS, Extrusion, High Impact
Information Provided by LG Chem
|
|||
| Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
|
Kingfa FRHIPS-8002 Flame Retardant Polystyrene
Features:UL 94 V-2 @ 1.0mm, V-2 @ 3.2mmExcellent balancing properties, Non-DPOExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElec..
|
|||
| Melt Temperature | <= 220 °C | <= 428 °F | |
|
Supreme Petrochem SP 246 Toughened Polystyrene
Characteristics Excellent clarity Very high toughness Deep drawability Improved thermal stabilityProcessing Extrusion ThermoformingApplications Thermoformed clear and deep draw products Rectangu..
|
|||
| Melt Temperature | <= 220 °C | <= 428 °F | |
|
Supreme Petrochem SP 266 Toughened Polystyrene
CharacteristicsGood stiffness Excellent toughness High flow Excellent clarity Processing Injection moldingApplications Transparent hangers Stationery items like pen barrels, geometric instruments ..
|
|||
| Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
|
Sax Polymers SAXLAC 120T Acrylonitrile Butadiene Styrene
Saxalac 120T is an antistatic, easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested ..
|
|||
| Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
|
Sax Polymers SAXLAC 310U Acrylonitrile Butadiene Styrene
Saxalac 310U is an antistatic, high impact resistant and light stabilized ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% ..
|
|||
| Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
|
Borealis Borcoat™ HE3453 Natural High Density Polyethylene for Steel Pipe Coating
Borcoat HE3453 is a natural and colorable high density polyethylene produced with the Borstar technology in similar conditions as the black ready made top coat Borcoat HE3450. Borcoat HE3453 is rec..
|
|||
| Melt Temperature | 220 - 245 °C | 428 - 473 °F | |
|
Lubrizol Isoplast® 2510 Engineering Thermoplastic Polyurethane Resin
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
|
|||
| Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
|
Tisan TISLAMID® 6 20% Glass Fiber Reinforced, Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Melt Temperature | <= 220 °C | <= 428 °F | |
|
Total PS CPDS 807 Flame Retardant Polystyrene
POLYSTYRENE (PS) COMPOUND (CPDS) 807 is a high impact flame retardant polystyrene for use in HGW applications. PS CPDS 807 can be supplied in both natural and colored forms.Main Characteristics:DBD..
|
|||
| Melt Temperature | 220 - 270 °C | 428 - 518 °F | |
|
Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced
Xmod GD301HP is reinforced with 32% chemically coupled glass fibers and based on specific Polymer matrix material which is bringing excellent mechanical properties (impact behavior) and very good st..
|
|||
| Melt Temperature | 220 - 230 °C | 428 - 446 °F | |
|
E-Polymers SEPAZ® LH50 PP Homopolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
|
|||
| Melt Temperature | 220 - 260 °C | 428 - 500 °F | Polymer Mass Temp |
|
Borealis Daplen™ EE103AE TPO Compound
Daplen EE103AE is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE103AE is a material with excellent impact /stiffness ratio. Thanks to its low ..
|
|||
| Melt Temperature | 220 - 250 °C | 428 - 482 °F | Extrusion Molding |
|
LG Chemical KEYFLEX BT S5035 Ester Type TPE
Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide..
|
|||
| Melt Temperature | 220 - 260 °C | 428 - 500 °F | Resin, Injection Molding |
|
LG Chemical LUTENE-H ME8000 HDPE
Description: LUTENE-H ME8000 is mainly intended for injection molding of containers. It has good mechanical properties and high productivity.Applications: Silicone cartridge, containers, complicated..
|
|||
| Melt Temperature | 220 - 230 °C | 428 - 446 °F | |
|
NOVA Chemicals Sclair® 11J4 Octene LLDPE Film Resin
(discontinued **)
Film Properties. Features: Low gel, excellent hermetic heat sealability, easy processability, high toughness and strength.Applications: Sealant web in food packaging, vacuum packaging, barrier appl..
|
|||
| Melt Temperature | 220 - 250 °C | 428 - 482 °F | |
|
Sax Polymers SAXALEN PPH304G25 Polypropylene Homopolymer, 25% Glass Filled
SAXALEN PPH304G25 is a 25% glass filled Polypropylene - Homopolymer intended for injection molding. This compound is characterized by high stiffness good impact resistance und reduced creep under lo..
|
|||