Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 300 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 270 - 300 °C
518 - 572 °F
Plastcom SLOVAMID 6 GF 60 000/1M PA6 reinforced with 60% glass fibre
Features: PA 6 for injection moulding, chemically strengthened with 60% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go..
Melt Temperature 270 - 300 °C
518 - 572 °F
Plastcom SLOVAMID 6 GF 65 PA6, 65% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
Melt Temperature 270 - 300 °C
518 - 572 °F
Plastcom SLOVAMID 6/66 GF 30 FRG 5 TS PA6/66, 30% glass fibre, flame retardant
FeaturesPA 6 + PA 66 alloy for injection moulding, chemically reinforced with 30 % glass fibre, with halogen and phosphorus free flame retardant. Main features: flammability in accordance with UL 94..
Melt Temperature 280 - 300 °C
536 - 572 °F
Plastcom SLOVAMID 66 BT LS PA66, basic type
FeaturesModified for general use, with excellent manufacturing properties, characterized by high strength and toughness also at minus temperatures. UV stabile. Used in automotive, electrical, engine..
Melt Temperature 280 - 300 °C
536 - 572 °F
Plastcom SLOVAMID 66 GF 10 GB 20 Polyamide 66, 10% Glass Fiber, 20% Glass Beads
FeaturesPA 66 chemically reinforced with 10% glass fiber and with the content of 20% glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can ..
Melt Temperature 280 - 300 °C
536 - 572 °F
Plastcom SLOVAMID 66 GF 20 GF 10 PA66, 20% glass fibre, glass beads
FeaturesPA 66 chemically reinforced with 20% glass fibre and with the content of 10 % glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can b..
Melt Temperature 280 - 300 °C
536 - 572 °F
Plastcom SLOVAMID 66 GF 20 PA66, 20% glass fibre
FeaturesChemically reinforced with 20 % glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. ..
Melt Temperature 275 - 300 °C
527 - 572 °F
Do not melt above 300°C
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66
Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char..
Melt Temperature 270 - 300 °C
518 - 572 °F
DuPont Performance Polymers Rynite® GW520CS NC010 PET  (Unverified Data**)
Rynite® GW520CS NC010 is a 20% glass fiber reinforced, flame retardant, color stabilized, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Melt Temperature 275 - 300 °C
527 - 572 °F
Do not melt above 300°C
Nilit Nilamid A3 H7 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H7 G6 is a 30% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc..
Melt Temperature 280 - 300 °C
536 - 572 °F
DAM; Injection Molding
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66  (Unverified Data**)
Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat..
Melt Temperature 280 - 300 °C
536 - 572 °F
ISO 294
Gromax BFG50-AH00B2 Nylon 6 50% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
Melt Temperature 275 - 300 °C
527 - 572 °F
Lavergne VYPET VNT 325 PET 25% Glass - Mineral Reinforced
Vypet 325 is a 25% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications.Features: High temperature performance; Good balance resilience-stiffne..
Melt Temperature 275 - 300 °C
527 - 572 °F
Lavergne VYPET VNT 835 PET 35% Glass-Mineral Reinforced
Vypet VNT 835 is a 35% mineral and fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional s..
Melt Temperature 275 - 300 °C
527 - 572 °F
Lavergne VYPET VNT 635A PET 35% Glass Reinforced
Vypet 635A is a 35 % glass reinforced PET injection molding compound designed for electrical and structural applications with a very glossy surface.Features: High temperature performance, Excellent..
Melt Temperature 260 - 300 °C
500 - 572 °F
ISO 294
Styrolution Luran® S KR2866C ASA / PC
Luran S KR2866C is a blend of ASA and PC with a reduced content of PC. It is characterized by a medium impact toughness and heat resistance.Good heat resistanceMedium impact strengthInformation prov..
Melt Temperature 280 - 300 °C
536 - 572 °F
Sax Polymers SAXAMID 226F3 Nylon 6.6, 15% Glass Fiber
SAXAMID 226F3 is a polyamide 6.6 injection-molding-grade reinforced with 15% glass fibers. This grade is suitable for applications requiring high strength and very good flow properties during proces..
Melt Temperature 270 - 300 °C
518 - 572 °F
Solvay Technyl® A 216 V40 40% Glass Filled Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Melt Temperature 280 - 300 °C
536 - 572 °F
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET
Information provided by A. Schulman.
Melt Temperature 280 - 300 °C
536 - 572 °F
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET
Information provided by A. Schulman.
Melt Temperature 280 - 300 °C
536 - 572 °F
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Melt Temperature 270 - 300 °C
518 - 572 °F
Toyobo GLAMIDE® TY-835TC Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Melt Temperature 280 - 300 °C
536 - 572 °F
DAM
DuPont Performance Polymers Zytel® PLUS PLS95G35DH1 BK031 Nylon
Zytel® PLS95G35DH1 BK031is a high flow 35% glass reinforced PA using SHIELD Technology, only from DuPont, combining excellent surface appearance, excellent welding and fatigue retention, exceptiona..
Melt Temperature 270 - 300 °C
518 - 572 °F
E-Polymers TEKANATE® G7020 General Purpose Easy Molding Polycarbonate
Modified Poly Carbonate: TEKANATE is a modified PC by improving polycarbonate resins with features of halogen-free flammability, transparency, impact resistance and reinforced fiberglass. It shows ..
Melt Temperature 280 - 300 °C
536 - 572 °F
BASF Petra® 7010 WT 7729 15% Glass Filled PET
Description: Petra 7010 WT7729 is a 15% glass fiber reinforced, pigmented white injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface ..
Melt Temperature 280 - 300 °C
536 - 572 °F
Injection-molding/Extrusion
BASF Ultramid® A3WG6 BK 00564 30% Glass Filled PA66 (Conditioned)
Description: 30% glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of high stiffness and dimensional stability such as lamp socket housings, f..
Melt Temperature 195 - 300 °C
383 - 572 °F
Average value: 221 °C Grade Count:25
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m..
Melt Temperature 260 - 300 °C
500 - 572 °F
DAM
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610  (Unverified Data**)
Zytel® RS 30G30HSL BK038A is a lubricated, heat stabilized, 30% glass fiber reinforced black polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on po..
Melt Temperature 270 - 300 °C
518 - 572 °F
BASF Ultramid® BU50I PA6 (Dry)
Description: Ultramid Ultratough Nylon BU50I is an unreinforced PA6, impact modified injection molding product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme ..
Copyright © lookpolymers.com All Rights Reserved