| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.61 g/cc | 0.0582 lb/in³ | ISO 1183 |
| Filler Content | 20 % | 20 % | |
| Melt Index of Compound | 17 g/10 min @Load 2.16 kg, Temperature 280 °C |
17 g/10 min @Load 4.76 lb, Temperature 536 °F |
cm3/10 min; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 145 MPa @Temperature 23.0 °C |
21000 psi @Temperature 73.4 °F |
ISO 527 |
| Elongation at Break | 2.5 % @Temperature 23.0 °C |
2.5 % @Temperature 73.4 °F |
ISO 527 |
| Tensile Modulus | 9.00 GPa @Temperature 23.0 °C |
1310 ksi @Temperature 73.4 °F |
ISO 527 |
| Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| Charpy Impact, Notched | 0.900 J/cm² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 251 °C | 484 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 1.8 MPa (264 psi) | 232 °C | 450 °F | ISO 75-1/-2 |
| UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746B |
| 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B | |
| 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746B | |
| UL RTI, Mechanical with Impact | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746B |
| 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B | |
| 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746B | |
| UL RTI, Mechanical without Impact | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B |
| 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746B | |
| 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746B | |
| Flammability, UL94 | V-2 @Thickness 0.750 mm |
V-2 @Thickness 0.0295 in |
IEC 60695-11-10 |
| V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
IEC 60695-11-10 | |
| V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
IEC 60695-11-10 | |
| V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
UL94 | |
| V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
UL94 | |
| V-2 @Thickness 0.750 mm |
V-2 @Thickness 0.0295 in |
UL94 | |
| Glow Wire Test | 900 °C @Thickness 0.750 mm |
1650 °F @Thickness 0.0295 in |
Ignition; IEC 60695-2-13 |
| 925 °C @Thickness 1.50 mm |
1700 °F @Thickness 0.0591 in |
Ignition; IEC 60695-2-13 | |
| 925 °C @Thickness 3.00 mm |
1700 °F @Thickness 0.118 in |
Ignition; IEC 60695-2-13 | |
| 950 °C @Thickness 0.750 mm |
1740 °F @Thickness 0.0295 in |
IEC 60695-2-12 | |
| 960 °C @Thickness 1.50 mm |
1760 °F @Thickness 0.0591 in |
IEC 60695-2-12 | |
| 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 200 V @Temperature 23.0 °C |
200 V @Temperature 73.4 °F |
IEC 60112 |
| 250 V @Temperature 23.0 °C |
250 V @Temperature 73.4 °F |
UL 746A |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 280 °C | 536 °F | Optimum |
| 270 - 300 °C | 518 - 572 °F | ||
| Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
| Drying Temperature | 120 °C | 248 °F | |
| Dry Time | 4.00 hour | 4.00 hour | |
| Moisture Content | <= 0.020 % | <= 0.020 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Natural Color | |
| Drying Recommended | Yes | |
| Filler | Glass fiber | |
| Forms | Pellets | |
| Generic | PET | |
| Material Status | Current | |
| Part Marking Code | >PET-GF20FR< | ISO 11469 |
| Polymer Family | Polyester | |
| Polymer Type | PET | |
| Processing Method | Injection Molding | |
| Product Category | Color Stable Resins | |
| Flame Retardant Resins | ||
| Glass Reinforced Resins | ||
| Region Available - Global | Yes | |
| Resin Identification | PET-GF20FR | ISO 1043 |
| RoHS Compliance | Contact Manufacturer |