Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom PLASTALEN® PQ 82 N Polypropylene with improved impact strength PP impact modified. General application in all industry branches. Delivered in natural mode and in the full RAL color scale. For injection molding.Information Provided by Plastcom spol. s r.o. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PC 51 C 30 Polypropylene Homopolymer and Copolymer, 30% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 30% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C... |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PC 59 GF 13 Compounded Polypropylene Homopolymer, 13% Chemically Coupled Glass Fiber FeaturesCompounded homopolymer PP, with the content of 13% chemically coupled glass fiber and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all indus.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PH 22 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Special designed for automotive light housings. Delivered in natural mo.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PH 51 T 30 PP, 30% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PH 63 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PH 99 GB 20 PP, 20% glass beads, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PQ 91T 5 PP, 5% mineral filling FeaturesModified PP for injection moulding with the content of 5 % mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Premix Thermoplastics PRE-ELEC® PP 1373 PRE-ELEC PP 1373 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
Polykemi AB POLYfill PP CPX10030 UV Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PC 93 T 5 PP reinforced with 5% mineral filler Features: Modified PP for injection moulding with the content of 5% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches.Packa.. |
|||
Melt Temperature | 240 - 250 °C | 464 - 482 °F | |
Samyang Triloy® 410N PC/PET alloy, Flame Retardant
(discontinued **) Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityFlame retardantApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang |
|||
Melt Temperature | 220 - 250 °C | 428 - 482 °F | Start Point: 240°C |
Kingfa HR-528 Modified ABS Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Melt Temperature | 220 - 250 °C | 428 - 482 °F | Start Point: 230°C |
Kingfa JH950-602 Low-temperature Resistant & Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surface, high glossApplications:ControllerPlug, socketShell of ammeterSmall hou.. |
|||
Melt Temperature | 220 - 250 °C | 428 - 482 °F | |
LG Chemical LI-921 ASA, Extrusion, High Stiffness Information Provided by LG Chem |
|||
Melt Temperature | 240 - 250 °C | 464 - 482 °F | |
LG Chemical LUMAX GP-5106F General Purpose PBT, 10% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Melt Temperature | 220 - 250 °C | 428 - 482 °F | |
LATI Laticonther 47/1 CP/80 PP Copolymer High thermal conductivity product based on Polypropylene copolymer (PPc). Special filler. Extrusion and molding injection grade.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
LATI Latilub 62-15ST PA6 Self-lubricating product based on Polyamide 6 (PA6). Silicone / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Term.. |
|||
Melt Temperature | 240 - 250 °C | 464 - 482 °F | |
LATI Latilub 75/4-15ST G/30 PBT, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polybutylene Terephthalate (PBT). Silicone / PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Melt Temperature | 180 - 250 °C | 356 - 482 °F | Injection molding |
Styrolution Styrolux® 693 D SBC Description: Styrolux® 693 D is a clear styrene-butadiene copolymer (SBC) with a well balanced combination of toughness and clarity. Styrolux® 693 D is mainly used for thermoformed articles, e.. |
|||
Melt Temperature | 235 - 250 °C | 455 - 482 °F | |
DuPont Surlyn® SG201U NC010 Supergloss Molding Alloy Surlyn® SG201U is a modified ionomer resin for applications that require a high gloss, molded in color surface color surface finish directly from the mold. The material is weatherable, durable, an.. |
|||
Melt Temperature | 240 - 250 °C | 464 - 482 °F | |
Eurostar Staramide BST42 PA6, Impact Modified, Injection Molded BST42 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MK001AS PP, Mineral Filled, Injection Molding Starpylen MK001AS is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MX05039 PP, Mineral Filled, Injection Molding Starpylen MX05039 is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MX06050 PP, 30% Glass Filled, Injection Molded Starpylen MX06050 is a 30% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MZ006S PP, Glass Fiber Filled, Injection Molded Starpylen MZ006S is a Glass fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WT 30GF S3)Information provided by Eurostar. |
|||
Melt Temperature | 240 - 250 °C | 464 - 482 °F | |
Eurostar Staramide BST03 PA6, Impact Modified, Injection Molded BST03 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
LATI Latiblend 6252 H2 G/30 PA6/PP Homopolymer Blend based on Polyamide 6 (PA6) / Polypropylene homopolymer (PPh). Heat stabilized. Glass fibers. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |