Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Kingfa Sci. & Tech. Co.
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Kingfa JH950-602 Low-temperature Resistant & Flame Retardant PC/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surface, high glossApplications:ControllerPlug, socketShell of ammeterSmall household appliance cabinetShell of chargerInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
<br>@Temperature 23.0 °C
1.17 g/cc
<br>@Temperature 73.4 °F
ASTM D792
Water Absorption 0.12 %
<br>@Temperature 23.0 °C,<br> Time 86400 sec
0.12 %
<br>@Temperature 73.4 °F,<br> Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
<br>@Temperature 23.0 °C
0.0040 - 0.0060 in/in
<br>@Temperature 73.4 °F
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength at Break >= 54.0 MPa
>= 7830 psi
50mm/min; ASTM D638
Elongation at Break >= 50 %
>= 50 %
50mm/min; ASTM D638
Flexural Strength 82.0 MPa
11900 psi
2mm/min; ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
2mm/min; ASTM D790
Izod Impact, Notched 4.50 J/cm
<br>@Thickness 3.20 mm,<br> Temperature -30.0 °C
8.43 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature -22.0 °F
ASTM D256
5.50 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
10.3 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 126 °C
<br>@Thickness 6.40 mm
259 °F
<br>@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
<br>@Thickness 6.40 mm
230 °F
<br>@Thickness 0.252 in
ASTM D648
Flammability, UL94 V-0
<br>@Thickness 3.20 mm
V-0
<br>@Thickness 0.126 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
ASTM D257
Dielectric Strength 28.0 kV/mm
711 kV/in
1.6mm; ASTM D149
Processing Properties Metric English Comments
Processing Temperature <= 265 °C
<= 509 °F
Rear Barrel Temperature 210 - 240 °C
410 - 464 °F
Start Point: 215°C
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Start Point: 225°C
Front Barrel Temperature 220 - 250 °C
428 - 482 °F
Start Point: 235°C
Melt Temperature 220 - 250 °C
428 - 482 °F
Start Point: 230°C
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Start Point: 60°C
Drying Temperature 100 - 110 °C
<br>@Time 14400 - 21600 sec
212 - 230 °F
<br>@Time 4.00 - 6.00 hour
Pre-dry
Back Pressure 0.000 - 1.00 MPa
0.000 - 145 psi
Descriptive Properties Value Comments
Injection Speed 60-100%