Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 85880 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 188 - 193 °C | 370 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 87358 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 87548 AS Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent PVC profile compound, with reduced surface resistivity, resulting in unlikely attraction and adhesion of dust. Actual results on surface resistivity = 1.3x10^15.Information provided by.. |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 87548 Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent PVC profile compound, with inherent water clear optical characteristics.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 87570 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 87771 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion L8230 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion L9630 Polyvinyl Chloride, Rigid (PVC, Rigid) Product can meet UL-94V-0. Material passed V-0 @ 1.5mm in screening test at PDI.Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ HTX 92052 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Melt Temperature | 174 - 193 °C | 345 - 379 °F | |
PolyOne Geon™ HTX Ultra LA425 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors below 50L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Ductile/Brittle transition as measured by Instrumented Impact is 5 de.. |
|||
Melt Temperature | 174 - 193 °C | 345 - 379 °F | |
PolyOne Geon™ HTX Ultra LA427Plus Polyvinyl Chloride Alloy (PVC Alloy) Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties based on Geon HTX Ultra LA427Plus Natural 0000Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ L4605 Green 5765 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid) Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Flexible BP90W2 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 188 - 193 °C | 370 - 379 °F | |
PolyOne Geon™ Vinyl Flexible XV3581G Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Geon™ Vinyl Flexible 86273 Trans 002 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Geon™ Vinyl Flexible 86280 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
Huntsman PE1903 EVA Film Extrusion
(discontinued **) 9% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent toughness and flexibility at low temperatures, and good heat-seal response.Applications: Film extrusion: laminating film, controll.. |
|||
Melt Temperature | 166 - 193 °C | 331 - 379 °F | Blown Film |
Chevron Phillips K-Resin® KR10 Styrene-Butadiene Copolymer, Film Grade
(discontinued **) Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: This SBC is easily processed on blown film or cast fi.. |
|||
Melt Temperature | 182 - 193 °C | 360 - 380 °F | with BUR of 2.4:1 or higher |
Westlake EF796 Low Density Polyethylene Westlake Polyethylene EF796 is a low density formulation suggested for film applications requiring a good balance of properties such as converter film for industrial packaging and general-purpose pa.. |
|||
Melt Temperature | 185 - 193 °C | 365 - 380 °F | |
Axiall 3014 Rigid PVC, Extrusion Georgia Gulf 3014 is a base for use of wood flour up to 40 percent. Impact Strength & ToughnessFlame RetardantChemical ResistanceDimensional StabilityInformation provided by Georgia GulfGeorgia Gul.. |
|||
Melt Temperature | 182 - 193 °C | 360 - 379 °F | |
Huntsman PE1403 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA Copolymer, DMF listed and FDA compliantFeatures: High clarity film with good toughness and flexibility at low temperatures.Applications: Film extrusion: frozen food and general .. |